LAIRD TFLEX HD93500

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

LAIRD TFLEX HD93500

Main features

  • 7.5 W/(m K) Thermal Interface
  • Compliant Silicone Gap Filler
  • Naturally Tacky Construction

Product Description

Tflex™ HD90500 is a 3500 um configuration within the Tflex™ HD90000 Series, a high-performance silicone thermal gap filler engineered for applications requiring efficient heat transfer and low mechanical stress on sensitive electronic components. The ceramic-filled silicone construction provides typical thermal conductivity of 7.5 W/m·K while maintaining high compliance for effective contact across uneven mating surfaces. Naturally tacky surfaces support placement during assembly without requiring an additional adhesive coating.

Key features

  • 7.5 W/m·K thermal conductivity for demanding electronics cooling applications.
  • Highly compliant silicone construction helps minimize stress while conforming to uneven surfaces.
  • Naturally tacky surfaces simplify installation without an additional adhesive layer.

Applications / Suitable for

  • Automotive electronics and ADAS modules
  • High-performance computing and networking equipment
  • Industrial power electronics
  • Telecommunications infrastructure

Technical Specifications

General Properties
Color
The color
Grey
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Ceramic Filled Silicone Sheet
Density (g)
3.5 g/cm3
Thickness range
3.5 mm
Thermal Properties
Operating Temperature
-65 to 125 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
7.5 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
8.73 x 10^13 Ohms⋅cm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical as-supplied properties of Tflex™ HD90500. This product is a part number within the Tflex™ HD90000 Series. Family-level properties are shown where applicable because the specific thickness for HD90500 is not identified in the supplied documentation.

Property Value Unit Method / Condition
Construction Ceramic-filled silicone gap filler — Tflex™ HD90000 Series
Color Grey — Visual
Nominal Thickness 3500 um HD90500 part number; thickness not identified in supplied documentation
Density 3.5 g/cm³ Typical
Hardness 500 and 750 μm: 45
1000 μm and up: 32
Shore 00 ASTM D2240
Surface Condition Naturally tacky on both sides — Standard construction
Shelf Life 2 years From date of shipment
Technical Properties

After-Processing / Final-State Properties

Typical installed properties of the Tflex™ HD90000 Series applicable to Tflex™ HD90500. Installed performance varies with compression, final bondline thickness, interface pressure, and mating surfaces.

Property Value Unit Method / Condition
Thermal Conductivity 7.5 W/m·K ASTM D5470
Operating Temperature -65 to 125 °C Continuous operating range
Volume Resistivity 8.73×1013 ohm·cm ASTM D257
Dielectric Constant 8.14 — ASTM D150 @ 1 MHz
Flammability UL 94 V-0 — UL 94
Outgassing Low outgassing — ASTM E595

 