LAIRD TFLEX 640

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

LAIRD TFLEX 640

Main features

  • 1.02 mm Thickness of Tflex 600 Series
  • 3.0 W/(m K) Thermal Interface
  • Naturally Tacky Surfaces

Product Description

Tflex™ 640 is the 1.02 mm-thick configuration of the Tflex™ 600 Series, an exceptionally soft and highly compliant silicone thermal gap filler designed to bridge interfaces between heat-generating components and adjacent cooling surfaces. The blue-violet pad uses a boron nitride-filled silicone construction to provide typical thermal conductivity of 3.0 W/m·K. Its naturally tacky surfaces support placement during assembly without requiring an additional adhesive coating.

Key features

  • 1.02 mm nominal thickness: Specific Tflex™ 600 Series configuration for controlled thermal-interface gaps.
  • Highly compliant construction: Soft silicone gap-filler design supports conformity around uneven component surfaces.
  • 3.0 W/m·K thermal conductivity: Supports heat transfer between electronic components and cooling hardware.
  • Naturally tacky surfaces: Helps hold the pad in position during assembly without a separate adhesive layer.

Applications / Suitable for

  • Automotive electronics, ADAS, infotainment, and ECU assemblies
  • Networking and telecommunications equipment
  • Portable and consumer electronics
  • Industrial and instrumentation electronics

Technical Specifications

General Properties
Color
The color
Blue Violet
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Ceramic Filled Silicone Sheet
Density (g)
1.34 g/cm3
Thickness range
1.02 mm
Thermal Properties
Operating Temperature
-45 to 200 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.0 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2 x 10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties of Tflex 6150 and its parent Tflex 600 Series. Values are provided for design guidance and are not guaranteed specifications.

Property Value Unit Method / condition
Construction and composition Ceramic-filled silicone sheet — Tflex 600 Series construction
Color Blue-violet — Visual
Nominal thickness 1.02 mm  Tflex 640 configuration; nominal uncompressed thickness
Density 1.30 g/cc Typical family-level value
Hardness 51 Shore 00 ASTM D2240
Surface condition Naturally tacky on both sides — Standard construction; one-side-tacky option is separately designated
Shelf life 2 years From date of shipment
Technical properties

After-processing / final-state properties

Typical family-level properties relevant to Tflex 6150 after placement within an assembled thermal interface. Installed performance varies with compression, final thickness, contact pressure, surfaces, and assembly design.

Property Value Unit Method / condition
Thermal conductivity 3.0 W/m·K ASTM D5470
Operating-temperature range -45 to 200 °C Documented Tflex 600 Series temperature range
Dielectric constant 3.3 — Typical family-level value; frequency not stated in the current product listing
Volume resistivity 2.0 × 1013 ohm·cm ASTM D257
Flammability rating V-0 — UL 94; confirm listing scope for the specific thickness and construction

 