LAIRD TFLEX 3200

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD TFLEX 3200

Main features

  • Low-Pressure Compliant Gap Filling
  • Tgard Dielectric Handling Layer
  • Reusable Low-Compression-Set Pad

Product Description

Tflex 3200TG Thermal Gap Filler is a 5.00 mm light-green filled silicone elastomer pad with a Tgard carrier for compliant thermal interfaces. The configured 457 x 457 mm sheet combines 1.2 W/(m K) thermal conductivity with Shore 00 hardness of 27 and one-sided surface adhesion. Its low compression set supports repeated pad use, while the carrier provides a cut-through-resistant dielectric handling layer. Applications include computers, telecommunications hardware, displays, memory modules, power conversion equipment, automotive electronics, LED lighting, and handheld devices.

Key features

  • 5.00 mm Configured Sheet: The 18 x 18 inch pad is supplied at the product-specific 5.00 mm thickness.
  • Tgard Dielectric Carrier: The carrier supports handling and provides a cut-through-resistant dielectric layer.
  • Reusable Compliant Interface: Low compression set supports repeated use while maintaining conformal component contact.

Applications / Suitable for

  • Computers, displays, and memory modules
  • Telecommunications and power conversion hardware
  • Automotive electronics, LED lighting, and handheld devices

Technical Specifications

General Properties
Color
The color
Light green
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Filled silicone elastomer on carrier line
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.79
Thermal Properties
Operating Temperature
(-)40 to 160 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.2 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied construction, dimensions, and handling properties for the 5.00 mm Tflex 3200TG sheet configuration.

Property Value Unit Method / condition
Construction Filled silicone elastomer on Tgard carrier Tflex 300TG series
Color Light green Visual
Configured thickness 5.00 mm 0.200 inch part configuration
Configured sheet size 457 x 457 mm 18 x 18 inch part configuration
Density 1.80 g/cc Configured product page
Hardness 27 Shore 00 ASTM D2240
Surface adhesion One side Tflex 300TG series
Shelf life 2 years from shipment Configured product page
Technical properties

After-processing / final-state properties

Typical thermal, electrical, temperature, and outgassing properties for Tflex 300TG; thermal resistance applies at the stated pressure.

Property Value Unit Method / condition
Thermal conductivity 1.2 W/(m K) ASTM D5470
Thermal resistance at 10 psi 1.59 deg C-in2/W Modified ASTM D5470
Operating temperature -40 to 160 deg C Typical range
Breakdown voltage Greater than 10,000 VAC ASTM D149
Coefficient of thermal expansion 600 ppm/deg C IPC-TM-650 2.4.24
Outgassing TML 0.56 % ASTM E595
Outgassing CVCM 0.10 % ASTM E595
Flammability UL 94 V-0 Typical property

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers