LAIRD RFLB/SS6M

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD RFLB/SS6M

Main features

  • Adhesive-Backed 0.51 mm Sheet
  • 10 MHz to 4 GHz Control
  • Greater Than 50 dB/cm Attenuation

Product Description

Eccosorb RF-LB RFLB/SS6M EMI Noise Suppression Absorber is a 0.51 mm grey silicone sheet with SS6M pressure-sensitive adhesive for localized low-frequency noise control. The configured 304.8 x 914.4 mm part covers 10 MHz to 4 GHz and has typical attenuation greater than 50 dB/cm at 2.5 GHz. Its flexible format supports placement over processors, memory, power ICs, circuit traces, flat cables, displays, and other radiating structures. Applications include control of surface currents, crosstalk, radiated emissions, unwanted coupling, and lower-microwave cavity resonances.

Key features

  • Thin Adhesive-Backed Placement: The 0.51 mm sheet uses an SS6M pressure-sensitive adhesive for localized installation.
  • Broad Low-Frequency Coverage: The configured absorber covers a documented 10 MHz to 4 GHz frequency range.
  • High Attenuation at 2.5 GHz: Typical attenuation is greater than 50 dB/cm at the stated frequency.

Applications / Suitable for

  • Processors, chipsets, memory, and power ICs
  • Circuit traces, high-speed lines, and flat cables
  • Surface-current, crosstalk, emission, and cavity-resonance control
Product Family

LAIRD RFLB/SS6M

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Grey
Density (g)
2.2 g/cm3
Thermal Properties
Service temperature
(-)70 to 177 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
7.45x10^11 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied construction, dimensions, and handling properties for the RFLB/SS6M 0.020 x 12 x 36 inch configuration.

Property Value Unit Method / condition
Resin system Silicone Configured RF-LB part
Color Grey Visual
Thickness 0.51 mm Configured part
Sheet size 304.8 x 914.4 mm Configured part
Density 2.20 g/cc Typical property
Hardness 70 with a tolerance of 10 Shore A Typical RF-LB data
Adhesive option SS6M PSA Configured part
Shelf life Minimum 365 days from shipment Typical property
Technical properties

After-processing / final-state properties

Typical electromagnetic, electrical, temperature, and outgassing properties for the configured RF-LB absorber; attenuation depends on frequency and installation.

Property Value Unit Method / condition
Frequency range 10 MHz to 4 GHz Configured part
Attenuation at 2.5 GHz Greater than 50 dB/cm Typical property
Permeability at 1 MHz 40 Typical property
Operating temperature -70 to 177 deg C Typical property
Volume resistivity 7.45 x 10^11 ohm cm Typical property
Outgassing TML 1.150 % Typical property
Outgassing CVCM 0.120 % Typical property
Flammability UL 94 H-B Configured part

Leading Brands Trust in Our Products and Services