LAIRD MF-117

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD MF-117

Main features

  • Machinable RF Component Stock
  • 2.8 to 119 dB/cm Attenuation
  • Sheets, Rods and Bars

Product Description

Eccosorb MF-117 Machinable RF Absorber Stock is rigid, magnetically loaded epoxy stock for machining RF and microwave absorbers, attenuators, and terminating elements. The material can be formed into stepped or tapered geometries for waveguide, coaxial, and stripline designs, allowing component dimensions to be refined during prototype evaluation. Standard MF stock is offered as sheets, rods, and bars, while typical MF-117 attenuation rises from 2.8 dB/cm at 1 GHz to 119 dB/cm at 18 GHz. Applications include terminations, attenuating elements, simple RF filters, antenna elements, and selected magnetic components.

Key features

  • Machinable Magnetic Epoxy: Rigid stock can be cut and shaped into application-specific RF and microwave components.
  • Multiple Stock Geometries: Sheets, rods, and bars support tapered, stepped, and compact component designs.
  • Frequency-Dependent Attenuation: Typical MF-117 attenuation increases substantially from 1 GHz through 18 GHz.

Applications / Suitable for

  • Waveguide, coaxial, and stripline terminations
  • RF and microwave attenuating elements
  • RF filters, antenna elements, and selected magnetic components
Product Family

LAIRD MF-117

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
<180 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.44 W/m.K
General Properties
Density (g)
1.6 - 4.9 g/cm3
Chemical Properties
Water Absorption
<0.3 %

Additional Information

Technical properties

As-supplied / before-processing properties

Standard Eccosorb MF stock forms and dimensions for machining MF-117 RF components.

Property Value Unit Method / condition
Construction Magnetically loaded epoxy Rigid machinable MF stock
Standard stock forms Sheets, rods, and bars Standard availability
Standard sheet size 30.5 x 30.5 cm Eccosorb MF sheets
Sheet thickness range 0.32 to 7.62 cm Standard listed thicknesses
Rod length 30.5 cm Standard rods
Rod diameter range 0.32 to 7.62 cm Standard listed diameters
Technical properties

After-processing / final-state properties

Typical Eccosorb MF series physical data and MF-117 attenuation values; installed performance depends on machined geometry and assembly design.

Property Value Unit Method / condition
Frequency range Greater than 1 GHz Typical Eccosorb MF series
Service temperature Less than 180 deg C Typical Eccosorb MF series
Thermal conductivity 1.44 W/(m K) Typical Eccosorb MF series
Attenuation at 1 GHz 2.8 dB/cm Typical MF-117 electrical properties
Attenuation at 3 GHz 11.0 dB/cm Typical MF-117 electrical properties
Attenuation at 8.6 GHz 46 dB/cm Typical MF-117 electrical properties
Attenuation at 10 GHz 56 dB/cm Typical MF-117 electrical properties
Attenuation at 18 GHz 119 dB/cm Typical MF-117 electrical properties