Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD CR-117

Main features

  • 100:3.2 Part A:B Mixing
  • 4 to 8 GHz Grade Range
  • ECCOSORB MF-117 Cured Equivalence

Product Description

ECCOSORB CR-117 is a two-part castable epoxy microwave absorber supplied as CR-117 Part A resin and ECCOSORB CR Part B catalyst. The CR-series technical data identifies CR-117 for a recommended 4-8 GHz range and a 100:3.2 Part A:Part B mix ratio by weight. Processing guidance recommends warming Part A and preferably the mold to about 65 deg C before blending, with vacuum degassing used when needed before casting. Documented uses include waveguide terminations, attenuators and loads, and localized RF-leakage potting.

Key features

  • Mix ratio: Two-part castable epoxy microwave absorber with a documented 100:3.2 Part A:Part B mix ratio by weight.
  • Key characteristic: CR-117 is identified in the CR-series technical data for a recommended 4-8 GHz frequency range.
  • Processing guidance: Warm Part A and preferably the mold to about 65 deg C before mixing.

Applications

  • Waveguide terminations
  • Attenuators and loads
  • Localized RF-leakage potting

Technical Specifications

Chemical Properties
Moisture absorption
0.1 %

Additional Information

RF & Microwave Absorbers

Castable RF absorption with CR-117 grade selection

ECCOSORB CR-117 is a two-part castable epoxy microwave absorber supplied as CR-117 Part A resin and ECCOSORB CR Part B catalyst. The CR-series technical data identifies CR-117 for a recommended 4-8 GHz range and a 100:3.2 Part A:Part B mix ratio by weight.

Two-part castable system100:3.2 by weight4-8 GHz grade range

As-Supplied System

CR-117 component and grade configuration

Keep the two supplied components and the recommended mix basis distinct from cured-material performance.

Item Documented value State / condition
Part A ECCOSORB CR-117 Part A resin As supplied
Part B ECCOSORB CR Part B catalyst As supplied
Recommended mix ratio 100:3.2 by weight Part A:Part B before casting
Recommended CR-117 frequency range 4-8 GHz Grade-selection guidance

Processing

Mix, degas and cast under the documented CR-series process window

Processing guidance recommends warming Part A and preferably the mold to about 65 deg C, then blending the two components. Entrapped air may be removed under vacuum when needed before casting.

Process controls

  • Part A:Part B ratio: 100:3.2 by weight.
  • Processing temperature guidance: about 65 deg C for warmed Part A and preferably the mold.
  • Approximate pot life: 30 minutes at 65 deg C.
  • Heat cure is required by the documented CR-series guidance; use the governing technical data for the complete cure schedule.

Applications

Documented RF absorber uses

Waveguide terminations

Cast absorber for molded waveguide terminations and related RF load structures.

Attenuators and loads

Cast configurations for attenuator and load applications identified in the supplier documentation.

Localized RF-leakage potting

Precise placement of small absorber volumes in or around documented RF-leakage areas.

Discuss ECCOSORB CR-117 processing and RF absorber selection

Contact Krayden for support evaluating CR-117 for the intended frequency range, casting geometry, mixing process and RF absorber configuration. Final process settings and cured performance should be confirmed against the governing technical source and the actual application design.