LAIRD CF500

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD CF500

Main features

  • X/Y/Z-axis conductive foam for EMI shielding and grounding
  • Low-compression gasket design with a typical 25-50% operating compression range
  • One-sided conductive PSA with die-cut, hole-punch, and notch customization

Product Description

Laird EcoFoam CF500 Series is a conductive foam gasket for EMI shielding and grounding in electronic equipment. The construction combines conductive foam with conductive pressure-sensitive adhesive, enabling X-, Y-, and Z-axis conductivity for enclosure and connector interfaces. Laird typically recommends 25% to 50% compression of the original gasket height, with the target depending on gasket size. The material can be customized by die-cutting, hole-punching, or notching. CF500 provides distinct operating-temperature and thickness options for applications including servers and cabinets, telecommunications equipment, displays, computers, and mobile devices.

Key features

  • Three-axis conductivity: X-, Y-, and Z-axis conductive foam supports EMI shielding and grounding.
  • Controlled compression: Laird typically recommends 25%-50% compression of original height, depending on gasket size.
  • Customizable format: Conductive PSA construction can be die-cut, hole-punched, or notched for application-specific geometry.
Product Family

LAIRD CF500

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature
-40 - 85 °C

Additional Information

Conductive foam gaskets

Laird EcoFoam CF500 Series

Laird EcoFoam CF500 Series is a conductive foam gasket for EMI shielding and grounding in electronic enclosures. Both use conductive foam with a conductive pressure-sensitive adhesive and provide X-, Y-, and Z-axis conductivity. The series can be converted for custom geometry, with CF500 offering different color, thickness, operating-temperature, and shielding-performance options.

Conductive foam + conductive PSA X/Y/Z-axis conductivity 25-50% recommended compression Custom die-cuttable CF500 and CF600 variants

Laird ShielderLaird EcoFoam conductive foam gasket for EMI shielding and grounding.

Conversion and fit

Design and installation considerations

EcoFoam is positioned for low-cycling EMI shielding and grounding applications and can be converted to suit enclosure geometry. Laird guidance emphasizes custom conversion, conductive PSA placement, and controlled gasket compression.

Custom conversion: Die-cutting, hole-punching, and notching are supported for custom shapes.
Attachment: The conductive foam construction is offered with conductive pressure-sensitive adhesive on one side for placement in the assembly.
Operating compression: Laird typically recommends compressing EcoFoam gaskets to 25% to 50% of original height; the appropriate value varies with gasket size.

 

CF500 and CF600 comparison

CF500 and CF600 share the EcoFoam conductive-foam format but differ in color, available thickness, operating temperature, and reported shielding test data. Use the variant-specific values below rather than treating the series as one uniform specification.

Variant Operating temperature Shielding effectiveness Selection note
CF500 Series -40 to 85 °C 98 dB average @300 MHz;
108 dB average @3 GHz
Gray conductive foam. The Laird product page lists 0.3, 0.5, 0.7, 1.0, 1.5, 2.0, 2.5, 3.0, and 4.0 mm thicknesses. Z-axis resistance is <0.2 Ω for CF520 on a 25 mm x 25 mm specimen at 50% compression.
CF600 Series -10 to 70 °C 60 dB average @1 GHz Black conductive foam. Datasheet foam thicknesses are 0.3, 0.5, 0.7, 1.0, 1.5, 2.0, 2.5, and 3.0 mm, designated CF603 through CF630. Z-axis resistance is <0.2 Ω under 50% compression.

Shielding-effectiveness results are reported at different frequencies and should not be read as a direct CF500-versus-CF600 performance ranking. The datasheets report average results using modified MIL-DTL-83528C. Both datasheets list a 12-month shelf life at 23 °C / 60% R.H.

Supported use contexts

Applications

Laird lists EcoFoam for electronic equipment where compressible shielding and grounding are needed around enclosure gaps, connectors, and similar interfaces. The use contexts below are directly supported for the CF500/CF600 family.

Servers and cabinets
Used for enclosure-level EMI shielding and grounding in server and cabinet assemblies, including low-cycling gasket interfaces.
Telecommunications equipment
Supported for telecommunications equipment where a customizable conductive foam gasket can be fit around enclosure or connector geometries.
Computers, displays, and mobile electronics
Laird lists televisions/displays, desktop and laptop computers, and tablets/smartphones as application areas for EcoFoam conductive foam.
Next steps

Evaluate EcoFoam CF500 for your EMI shielding design

Krayden can help review the required gasket geometry, compression target, operating temperature, thickness, and shielding/grounding requirements for your enclosure. Contact our team to discuss CF500 versus CF600 selection, custom converting needs, and integration into low-cycling connector or enclosure designs.