LAIRD BSR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD BSR

Main features

  • 6-18 GHz cavity-resonance control
  • Flexible, electrically non-conductive silicone construction
  • 0.47% TML / 0.28% CVCM outgassing values

Product Description

Laird Eccosorb™ BSR is a thin, flexible, magnetically loaded silicone microwave absorber designed for cavity-resonance control from 6 to 18 GHz. The electrically non-conductive material combines high magnetic loss with a -40 to 170°C service-temperature range and documented low-outgassing data. It can be installed directly in front of metallic surfaces, cut to shape, and conformed to curved geometries. BSR is available in BSR-1 and BSR-2 versions, with multiple thicknesses and optional pressure-sensitive adhesive configurations.

Key features

  • 6-18 GHz cavity-resonance absorber: Current Laird product positioning covers 6 to 18 GHz for cavity-resonance control.
  • Flexible silicone construction: The thin elastomeric sheet can be cut to shape and conformed to compound curves.
  • High-temperature service: Documented service-temperature range is -40 to 170°C.
  • Electrically non-conductive: Current product data lists volume resistivity of 2 x 108 ohm-cm.
  • Documented outgassing data: 0.47% TML and 0.28% CVCM are reported per ASTM E595-07.
  • Attachment flexibility: Available with or without a pressure-sensitive adhesive option.

Applications / Suitable for

  • Cavity-resonance damping, surface-current control, coupling reduction, and reflection damping in microwave assemblies.
  • Microwave terminations, loads, attenuators, waveguides, and transmission systems.
  • Aerospace, defense, space, power-amplifier, oscillator, and down/up-converter applications.
Product Family

LAIRD BSR

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature
-40 to 170 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
50 %
General Properties
Density (g)
4.2 g/cm3
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
0.39 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2 x 10^9 Ohms⋅cm
Chemical Properties
Water Absorption
<0.1% %

Additional Information

Cavity resonance absorber

Laird Eccosorb™ BSR

Laird Eccosorb BSR is a flexible silicone elastomer absorber for cavity-resonance and EMI control in microwave assemblies. Current Laird product data positions BSR for 6-18 GHz operation with 40 dB/cm attenuation at 10 GHz, an electrically non-conductive construction, and a -40 to 170°C operating-temperature range.

6-18 GHz 40 dB/cm at 10 GHz -40 to 170°C Silicone elastomer Electrically non-conductive UL94 V-0

Laird Eccosorb BSR high-loss silicone elastomer microwave absorber sheet.

Material and formats

Material and configuration

Construction
Flexible silicone sheet
Black, magnetically loaded elastomeric absorber that can conform to compound curves.
Version mapping
BSR-1 / BSR-2
BSR-1 corresponds to MFS-124 and BSR-2 corresponds to MFS-117.
Listed thickness range
0.25-12.70 mm
Current Laird product data lists minimum and maximum thickness values across available BSR configurations.
Attachment options
PSA available
Configurations are available with or without pressure-sensitive adhesive, with on-drawing options also listed by Laird.
Installation

Placement and conversion guidance

Eccosorb BSR is designed to function directly in front of a metallic surface. Its flexible sheet form can be cut and fitted to contoured geometry; bonding method should be selected with the intended service temperature in mind.

Placement: Install the absorber directly in front of a metallic surface for the intended absorber function.
Cutting and forming: The sheet can be cut with a sharp knife and template and can conform to contoured surfaces.
High-temperature bonding: For service temperatures above 121°C (250°F), Laird instructs bonding to most substrates with an RTV silicone-based adhesive used with a suitable primer.

Illustrate BSR installed directly in front of a metallic surface and cut to fit the target geometry.

Technical data

Performance properties

Values are typical design guidance unless noted. Application performance can vary with geometry, thickness, placement, and operating conditions, so material should be evaluated in the intended assembly.

Property Value Unit Method / condition
Product frequency range 6-18 GHz Current Laird product positioning
Attenuation 40 dB/cm At 10 GHz
Service temperature -40 to 170 °C Documented service / operating range
Volume resistivity 2 x 108 ohm-cm Current Laird product data
Hardness >70 Shore A Typical
Tensile strength 5.0 MPa Typical
Density 4.2 g/cc Typical
Elongation 50 % Typical
Thermal expansion 63 x 10-6 per °C Typical
Thermal conductivity 0.865 W/mK Typical
Water absorption <0.1 % 24-hour value
Outgassing 0.47 / 0.28 % TML / % CVCM ASTM E595-07
Flammability rating UL94 V-0 - Current Laird product data
Compliance RoHS / REACH - Current Laird product data: compliant / yes
Use contexts

Applications

BSR is used where a flexible, non-conductive microwave absorber can be placed near metal to damp cavity resonance, surface currents, coupling, and reflections within its documented frequency range.

Microwave cavities and enclosed RF assemblies
Eccosorb BSR is engineered to reduce or eliminate surface currents, cavity resonance, and coupling while damping reflections. Its magnetic-loss behavior and 6-18 GHz positioning make it relevant for evaluating unwanted resonant energy in metallic microwave housings and cavities.
Terminations, loads, attenuators, and waveguides
Laird identifies microwave terminations, loads, attenuators, waveguides, and transmission systems as supported use contexts. The cuttable, conformable sheet format allows the absorber to be shaped for the available internal geometry and positioned near metallic surfaces.
Aerospace, defense, and space RF electronics
Laird recommends BSR/MFS for high-reliability aerospace, military, and space applications. Its documented outgassing values, electrically non-conductive silicone construction, and -40 to 170°C service range provide concrete screening criteria for RF hardware in demanding environments.
Product resource

Product resources

Laird Eccosorb Microwave Absorber Commercial Brochure
This supplier brochure provides a broader Eccosorb absorber selection overview, including frequency-range positioning, cavity-resonance product families, manufacturing and testing capabilities, and reference use cases. It positions Eccosorb BSR as a 6-18 GHz high-loss flexible absorber sheet.
Next steps

Evaluate Eccosorb BSR for your RF assembly

Krayden can help review frequency range, cavity geometry, thickness and format, attachment method, and service temperature when evaluating Eccosorb BSR for cavity-resonance and EMI-control applications. Contact us to discuss available configurations, sampling, conversion needs, or technical questions for your specific assembly.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers