KESTER 1429

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

KESTER 1429

Main features

  • VOC-Free Water-Based Fluxing
  • Self-Neutralizing Post-Solder Residue
  • Water-Only Residue Removal

Product Description

Kester 1429 VOC-Free Organic Water-Soluble Liquid Flux is a water-based, high-activity flux for tinning, dipping, and soldering processes that require water-removable residues. Its self-neutralizing chemistry develops a neutral, non-corrosive residue when properly heated, while adjusted surface tension supports solder flow and control of icicling and bridging. The ORH1 flux contains a typical 18% solids and can be applied by spray, dip, or wave methods. It may be used without preheating and can be diluted for supported applications. Applications include tinning and dipping operations and soldering tasks where rosin flux is too inactive and inorganic acid flux is too corrosive.

Key features

  • VOC-Free Water-Based Flux: Water-based ORH1 chemistry provides high activity without an organic-solvent carrier.
  • Water-Removable Residue: Residue can be removed with water without neutralizers, saponifiers, or detergents.
  • Self-Neutralizing Chemistry: Proper heating develops a neutral, non-corrosive residue with no SIR degradation.

Applications / Suitable for

  • Tinning and dipping operations
  • Spray, dip, or wave fluxing
  • Water-wash soldering processes

Technical Specifications

General Properties
Solids
18 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.061 ± 0.010 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-flux properties and handling limits before soldering.

Property Value Unit Method / condition
Flux classification ORH1 J-STD-004
Specific gravity 1.061 +/- 0.010 At 25 deg C
Typical solids 18 % J-STD-004; IPC-TM-650 Method 2.3.34
Chloride and bromides 2.3 % IPC-TM-650 Method 2.3.35
Minimum storage temperature 4 deg C Water-based formulation
Shelf life 2 years Stored at 4 to 25 deg C

Leading Brands Trust in Our Products and Services