Hysol GR910-C4 |Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR910-C4 |Black Epoxy Mold Compound

Main features

  • Improved version of GR910-C
  • Lower smile warpage
  • Smaller cut size (53um)

Product Description

Hysol GR910-C4 is an improved version of GR910-C. This black, epoxy, semiconductor grade molding compound is designed for Memory ball grid arrays (BGA) and land grid arrays (LGA). Its small spherical silica cut (cut size of 53um), offers high fluidity and low smile shrinkage that aids a very advanced warpage control.

There are two main differences between Hysol GR910-C4 and GR910-C.

  1. The first one is the filler cut size: C4 cut size is 53microns; C cut size is 75 microns. When a package design has very narrow gaps (100microns), C4 will be a better candidate and have better filling performance than C.
  2. The second and maybe most important difference between them is the warpage performance. C4 has smaller smile warpage than C with everything that entails.

Hysol GR910-C4 is a halogen free, environmentally friendly compound with good electrical performance that meets UL 94 V-0 Flammability at 1/8 inch thickness. Main features are summarized:

Moldability (Check the test results)

  • Small filler cut (53um) to have good filling performance
  • Good fluidity to prevent wire sweep (W/S) failures

Reliability 

  • Low shrinkage ratio
  • Low moisture absorption
  • Excellent warpage control during PMC and reflow process
  • Meet MSL3 @260°C requirements
  • Proven reliability performance on BGA/LGA package 

Check the BGA package key considerations. 

Check GR910 series comparison

Technical Specifications

General Properties
Color
The color
Black
Filler Content
88 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
30000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.3 %
Physical Properties
Spiral Flow @ 175°C
170 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
130 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1 W/m.K
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
7 - 15 s

Additional Information

BGA Packaging Key Considerations

GR910 Series Product Comparison

GR900 Series Molding Results At Customers' Sites

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers