Product Description

HumiSeal® 1A33/521 PB25 Urethane Conformal Coating is a single-component polyurethane conformal coating pre-blended to 25 cP for immediate use in automated spray equipment without additional thinning. Designed for general printed circuit board applications, it provides protection against moisture, salt and corrosive environments, dirt, and other supported environmental exposure. The flexible coating dries to handle in 15 minutes, fluoresces under UV light for inspection, and is readily repairable. Recommended dry-film thickness is 25–75 microns, with optional cure schedules of 30 days at room temperature, 30 hours at 76°C, or 20 hours at 88°C to reach optimum properties.

Key features

  • Ready-to-spray 25 cP pre-blend: Formulated for automated spray equipment without additional thinning.
  • Single-component polyurethane: Provides a flexible cured conformal coating for general printed circuit board applications.
  • Fast handling: Typical drying time to handle is 15 minutes.
  • UV inspection and repair: Fluoresces under UV light for coverage inspection and is readily repairable.
  • Environmental protection: Supports protection against moisture, salt and corrosive environments, and dirt.
  • Qualified 1A33 coating system: The 1A33 system meets multiple military, IPC, IEC, UL, REACH, RoHS, and salt-spray requirements.

Applications / Suitable for

  • Automated spray coating of printed circuit board assemblies
  • Protection of electronics from moisture, salt, corrosive environments, and dirt
  • UV-inspectable conformal coating processes
  • Repairable polyurethane coating for general PCB applications
Product Family

HUMISEAL 1A33/521PB25

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Coating Thickness
25-75 nm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
26 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
7,500 V

Additional Information

Conformal Coatings | Spray-Ready Polyurethane

HumiSeal® 1A33/521 PB25 Urethane Conformal Coating

HumiSeal 1A33/521 PB25 is a single-component polyurethane conformal coating pre-blended for automated spray application without additional thinning. It combines fast handling, flexible environmental protection, UV-fluorescent inspection, repairability, and documented electrical and thermal performance.

25 ± 3 cP 36 ± 1% solids 15 min handle 25–75 µm thickness UV fluorescent

Product data

As-Supplied Properties

Typical exact-product liquid-coating data. Values are representative and are not specifications.

Property Value Unit Method / condition
Product type Single-component polyurethane conformal coating — Pre-blended for automated spray
Viscosity 25 ± 3 cP Fed-Std-141, Method 4287
Solids content 36 ± 1 % by weight Fed-Std-141, Method 4044
Density 0.93 ± 0.02 g/cm³ ASTM D1475
Volatile organic compounds 569 g/L Exact-product HumiSeal TDS
Drying time to handle 15 min Fed-Std-141, Method 4061
Shelf life 24 months At room temperature from date of manufacture
Application

Surface Preparation, Spraying, and Cure

Cleanliness is critical to conformal-coating performance. Surfaces must be free of moisture, dirt, wax, grease, flux residues, and other contaminants. Confirm compatibility with the actual assembly materials, process conditions, and cleanliness level before production use.

Application: Use in automated spray equipment without additional thinning; equipment settings and spray pressure must be validated for the process.
Recommended coating thickness: Apply a dry-film thickness of 25–75 microns.
Optional cure schedules: Reach optimum properties after 30 days at room temperature, 30 hours at 76°C, or 20 hours at 88°C.

Conformal Coating Sequence

Stage 1
Clean and validate the assembly
Remove moisture, dirt, wax, grease, flux residues, and other contaminants. Assemblies using low-residue no-clean materials may be coated only after adequate compatibility testing confirms the assembly materials, process, and cleanliness level.
Stage 2
Apply the spray-ready pre-blend
Spray HumiSeal 1A33/521 PB25 without additional thinning using automated equipment. Control coverage, wet film, spray pressure, atomization, masking, and ventilation to produce a uniform 25–75 micron dry film.
Stage 3
Cure, inspect, and release
Allow the coating to dry and complete the selected cure schedule. Inspect coverage under UV light, confirm the required thickness and workmanship, and release the assembly only after the validated cure and inspection criteria are satisfied.
Final protective film

Cured Coating Properties

Typical properties of fully cured HumiSeal 1A33 and its pre-blends. Values are representative and should not be used as design allowables.

Property Value Unit Method / condition
Recommended dry-film thickness 25–75 µm Documented application range
Thermal shock -65 to 125 °C 50 cycles per MIL-I-46058C
Coefficient of thermal expansion 193 ppm/°C TMA
Glass transition temperature 26 °C DSC
Modulus 27.2 MPa DMA at 40°C
Flammability V-0 — UL 94
Dielectric withstand voltage >1,500 V MIL-I-46058C
Dielectric breakdown voltage 7,500 V ASTM D149
Dielectric constant 3.6 — 1 MHz and 25°C; ASTM D150-98
Dissipation factor 0.03 — 1 MHz and 25°C; ASTM D150-98
Insulation resistance 2.0 × 1014 Ω MIL-I-46058C
Moisture insulation resistance 1.6 × 1010 Ω MIL-I-46058C
Comparative tracking index PLC 0 — UL746E at 600 V
Fungus resistance Passes — ASTM G21
Storage and Handling

Store HumiSeal 1A33/521 PB25 away from excessive heat or cold in tightly closed containers at 0–35°C. Before use, allow the product to equilibrate for 24 hours at 18–32°C. The solvent system is flammable: keep the material away from open flames, sparks, heat, and other ignition sources, control static electricity, and use adequate ventilation to carry vapors and spray mist away from operators. Consult the current SDS before handling, application, storage, transport, spill response, or disposal.

Qualifications and Compliance

Requirement Product status Scope note
MIL-I-46058C Meets HumiSeal 1A33 coating requirement; fully cured pre-blends are documented as equivalent.
IPC-CC-830B Meets HumiSeal 1A33 coating requirement.
IEC60664-3 Meets HumiSeal 1A33 coating requirement.
UL746E and UL94 V-0 Meets UL recognition is listed under file number E105698.
REACH and RoHS Directive EU 2015/863 Compliant Confirm current regional obligations and customer-specific declaration requirements.
IEC61086 / IEC60068-2-11 salt spray Passes HumiSeal 1A33 coating-system test statement.

Inspection, Compatibility, and Rework

UV inspection and repair
The cured coating fluoresces under UV light to support coverage inspection and is documented as readily repairable. HumiSeal Stripper 1063 is the recommended stripper. Define the UV source, inspection criteria, masking, repair method, and post-rework cleanliness requirements within the manufacturing process.
Cleanliness, materials, and chemistry
The 1A33 system contains no free isocyanates and is documented for low moisture-vapor permeability and excellent chemical resistance. These statements do not establish universal compatibility with every substrate, component, flux, no-clean residue, cleaning process, or chemical exposure; validate the actual assembly and environment.
Supported use contexts

Applications

HumiSeal 1A33/521 PB25 supports printed circuit board coating processes where the assembly materials, cleanliness, spray equipment, coating thickness, cure schedule, inspection method, and service environment have been validated.

Automated PCB conformal coating
Use the ready-to-spray 25 cP pre-blend in validated automated spray equipment to produce a uniform 25–75 micron protective film.
Moisture and corrosive-environment protection
Protect compatible assemblies against moisture, salt and corrosive environments, dirt, and related supported environmental exposure.
Inspectable and repairable coating processes
Use UV fluorescence to inspect coverage and apply the validated HumiSeal repair or Stripper 1063 rework process where correction is required.
Next steps

Technical Support

Work with Krayden to evaluate HumiSeal 1A33/521 PB25 against your PCB materials, flux and cleanliness condition, masking plan, automated spray equipment, target thickness, cure schedule, UV inspection criteria, repair process, and service environment. Our team can help review compatibility, process trials, packaging, and implementation requirements.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers