FCT NL932

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

FCT NL932

Main features

  • Halide-Free ROL0 Flux
  • Nine-Month Refrigerated Shelf Life
  • SAC305 and SN100C Options

Product Description

FCT NL932 No-Clean Lead-Free Solder Paste is a halide-free no-clean lead-free solder paste for SMT printing and reflow in air or nitrogen. It is available with SAC305 and SN100C alloys using Type 3 or Type 4 powder, with Type 5 available by request. The NC32 flux system is supplied in jars, cartridges, syringes, and enclosed print-head formats. Refrigerated storage at 0 to 10 deg C provides a shelf life greater than nine months, while the working temperature range is 19 to 32 deg C and stencil life exceeds eight hours under the stated conditions.

Key features

  • Halide-free no-clean flux: The NC32 flux supports no-clean processing with ROL0 classification and zero-halide test results.
  • Extended refrigerated shelf life: Storage at 0 to 10 deg C provides more than nine months of shelf life.
  • SAC305 and SN100C options: The paste is available with both lead-free alloy systems in multiple powder sizes.

Applications

  • Lead-free SMT solder-paste printing
  • Reflow in air or nitrogen
Product Family

FCT NL932

Loading pricing…

Technical Specifications

Other Properties
Stencil Life
Period during which solder paste remains usable on a stencil for printing
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Flux, alloy, powder, storage, working-range, and stencil-life data before reflow.

Property Value Unit Method / condition
Flux system NC32 - No-clean flux
Flux classification ROL0 - J-STD-004A
Halide test result 0.00 % Zero-halide result
Alloy options SAC305 and SN100C - Standard product availability
Powder size Type 3 or Type 4; Type 5 by request - Product configuration
Metal loading 88.30 % SAC305 and SN100C, Type 3 and Type 4
Refrigerated storage 0 to 10 deg C Recommended storage range
Shelf life > 9 months At 0 to 10 deg C
Room-temperature exposure Up to 2 weeks Paste storage outside refrigeration
Working temperature range 19 to 32 deg C Paste processing range
Stencil life > 8 h At 20 to 25 deg C under the stated humidity condition