FCT NL930PT

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

FCT NL930PT

Main features

  • ROL0 Zero-Halide Flux
  • Eight-Hour Stencil Life
  • Multiple Lead-Free Alloy Options

Product Description

FCT NL930PT No-Clean Lead-Free Solder Paste is a no-clean lead-free solder paste with pin-testable flux residue for SMT printing and reflow. The flux system is classified ROL0 and is stated with 0.0% halide ion and halogen content. Available alloy options include SAC305, SN100C, Sn96.5/Ag3.5, SN100CV, LF-C2, and anti-tombstoning mixtures in supported powder sizes. The paste is formulated for fine-pitch and small-area-ratio apertures, provides an 8 hour stencil life under the stated temperature and humidity conditions, and supports reflow within approximately 8 hours after printing.

Key features

  • ROL0 zero-halide flux: The flux classification is ROL0 with 0.0% documented halide ion and halogen content.
  • Eight-hour stencil life: The paste maintains a documented stencil life under controlled temperature and humidity.
  • Multiple lead-free alloy options: Supported configurations include SAC305, SN100C, SN100CV, LF-C2, and Sn96.5/Ag3.5.

Applications

  • Lead-free no-clean SMT solder-paste printing and reflow
Product Family

FCT NL930PT

Loading pricing…

Technical Specifications

Other Properties
Stencil Life
Period during which solder paste remains usable on a stencil for printing
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Flux, alloy, powder, stencil-life, and handling data before reflow.

Property Value Unit Method / condition
Physical form Paste - As supplied
Flux classification ROL0 - J-STD-004B
Halide ion content 0.0 wt % IPC 2.3.28.1
Halogen content 0.0 wt % EN 14582 and IPC 2.3.28.1
Solder alloy options SAC305; SN100C; Sn96.5/Ag3.5; SN100CV; LF-C2; anti-tombstoning mixtures - Powder size varies by alloy and configuration
Solder powder types Type 3 or 4; Type 5 size range stated - Availability depends on alloy/configuration
Stencil life 8 h At 18 to 29 deg C and 10 to 70% RH
Warm-up time 3 to 4 h Sealed container to 18 to 29 deg C before use
Printed-board hold time Approximately 8 h Reflow as soon as practical after printing