EPOXYLITE MR101

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

EPOXYLITE MR101

Main features

  • Thixotropic Minimal-Flow Masking
  • Fifteen-to-Thirty-Minute Air Dry
  • High-Temperature Dry-Film Stability

Product Description

EPOXYLITE MR 101 Masking Grease is a light-brown, grease-like masking compound containing volatile solvents for protecting surfaces that should remain uncoated during painting or varnishing. Its thixotropic consistency limits flow after placement, and the applied material air dries in 15 to 30 minutes. The dry masking film is stated not to affect the cure of paint or varnish and remains stable at temperatures up to 500 deg C. The compound is supplied for temporary process protection and is described as easy to remove after the coating operation.

Key features

  • Thixotropic masking placement: The grease-like compound minimizes flow on protected areas.
  • Fifteen-to-thirty-minute air dry: The applied masking material develops a dry film within the documented time range.
  • High-temperature dry-film stability: The dried masking film is reported stable up to 500 deg C.

Applications

  • Masking surfaces that should not be coated during painting or varnishing
Product Family

EPOXYLITE MR101

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
Below 25 °C
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
26 °C
Physical Properties
VOC
6.4 pounds / gallon

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical, volatile-content, and storage data for the masking compound.

Property Value Unit Method / condition
Appearance Light-brown grease-like compound - As supplied
Flow behavior Thixotropic - Minimal flow after placement
Nonvolatile content 20 % Typical as-supplied value
Weight per gallon 7.9 to 8.2 lb/gal As supplied
Flash point 26 (79) deg C (deg F) Product value
Volatile organic content 6.4 lb/gal ASTM D3960
Shelf life 12 months Under stated storage conditions
Technical properties

After-processing / final-state properties

Typical dry-film and removal characteristics. Values are not guaranteed specifications.

Property Value Unit Method / condition
Dry-film temperature stability Up to 500 (932) deg C (deg F) Stability limit
Effect on coating cure Does not affect cure - Dry film with paint or varnish
Removal characteristic Easy to remove - Masking-process characteristic

Leading Brands Trust in Our Products and Services