Huntsman Epocast 50A1/9816

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Huntsman Epocast 50A1/9816

Main features

  • Two-Component Epoxy System
  • 7,770 mPa s Resin Viscosity
  • EPOCAST 50-A1/Hardener 9816 System

Product Description

EPOCAST® 50-A1 Resin with Hardener 9816 is a two-component epoxy material system comprising EPOCAST® 50-A1 epoxy resin and Hardener 9816. The resin is supplied as an epoxy constituent with a reported dynamic viscosity of 7,770 mPa·s at 20°C and density of 1.2 g/cm³ at 25°C. Hardener 9816 is a lower-viscosity curing component with a reported dynamic viscosity of 250 mPa·s and density of 1.02 g/cm³ at 25°C. The supplied resources do not establish the mix ratio, working life, cure schedule, supported substrates, applications, or cured performance of the combined system.

Key features

  • Two-component epoxy system: Combines EPOCAST® 50-A1 epoxy resin with Hardener 9816 as separate resin and curing components.
  • Resin viscosity: EPOCAST® 50-A1 has a reported dynamic viscosity of 7,770 mPa·s at 20°C.
  • Low-viscosity hardener: Hardener 9816 has a reported dynamic viscosity of 250 mPa·s at 25°C.

Technical Specifications

General Properties
Color
The color
Amber
Density
Volumetric mass per unit
1.18 kg/m3
Physical Properties
Viscosity (Part B)
7,770 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Reported physical properties of the individual EPOCAST® 50-A1 resin and Hardener 9816 components. These SDS values are not presented as product specifications.

Property Value Unit Method / condition
Component function Epoxy constituent / hardener — EPOCAST® 50-A1 resin / Hardener 9816
Dynamic viscosity 7,770 / 250 mPa·s EPOCAST® 50-A1 at 20°C / Hardener 9816 at 25°C
Density 1.2 / 1.02 g/cm³ EPOCAST® 50-A1 / Hardener 9816; 25°C
Relative density 1.21 / 1.02 — EPOCAST® 50-A1 / Hardener 9816
Water solubility Partly soluble / practically insoluble — EPOCAST® 50-A1 / Hardener 9816; 20°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers