EPOCAST 1656

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1656

Main features

  • Low-Density Potting Material
  • Paste Consistency for Application
  • Long Work Life

Product Description

EPOCAST® 1656-A/B is a two-component, low-density epoxy syntactic compound with a thick-paste consistency and a 50–90 minute gel time at 25°C. The mixed system has a typical density of 0.80 g/cm³ and may be cured for seven days at room temperature or gelled at room temperature followed by 2–3 hours at 66°C. It is used as a core fill for metal skins to add stiffness and strength to fabricated parts and is also suitable for core splicing and reinforcing radii and corners in reinforced-plastic structures. EPOCAST® 1656-A/B meets GM-4006-1-2 requirements.

Key features

  • Low-density mixed system: Typical mixed density of 0.80 g/cm³ supports lightweight structural filling applications.
  • Thick paste with long work life: Paste consistency is combined with a typical 50–90 minute gel time for a 100 g mass at 25°C.
  • Temperature-dependent strength data: Cured compressive-strength results are documented from −55°C to 177°C.

Applications / Suitable for

  • Core filling for metal skins in fabricated structural parts
  • Core splicing
  • Strengthening radii and corners in reinforced-plastic structures

Technical Specifications

General Properties
Color
The color
Light Tan
Density (g)
0.8 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received and processing data. Component order is Part A resin / Part B hardener / mixed system where multiple values are shown.

Property Value Unit Method / condition
Color Light tan / amber / light tan — Part A / Part B / mixed; visual
Density 0.80 / 1.00 / 0.80 g/cm³ Part A / Part B / mixed; ASTM 1622
Viscosity or consistency Part A: paste; Part B: 500 cP; mixed: paste — 25°C; ASTM D2196
Gel time 50–90 min 100 g mixed mass at 25°C; ASTM D2471
Mix ratio by weight 100:12 parts Part A resin : Part B hardener
Material temperature before mixing Above 18 °C Condition both components before mixing
Cure schedule 7 days at 25°C; or gel at 25°C followed by 2–3 hours at 66°C — Supplier-listed cure options
Shelf life 6 months Unopened at 25°C; store sealed and dry at 2–40°C away from direct sunlight
Technical properties

After-processing / final-state properties

Typical cured properties provided for product evaluation and not for specification purposes. Values apply only to the listed test methods and conditions.

Property Value Unit Method / condition
Tensile lap shear 700 (4.8) psi (MPa) ASTM D1002; etched aluminum/aluminum; 25°C
Compressive strength at −55°C 9,500 (65.5) psi (MPa) ASTM D695; measured at 2% strain
Compressive strength at 25°C 8,000 (55.2) psi (MPa) ASTM D695; measured at 2% strain
Compressive strength at 83°C 3,000 (20.6) psi (MPa) ASTM D695; measured at 2% strain
Compressive strength at 177°C 550 (3.8) psi (MPa) ASTM D695; measured at 2% strain
Flatwise tensile strength at 23°C 2,000 (13.8) psi (MPa) ASTM C297
Flatwise tensile strength at 71°C 1,000 (6.9) psi (MPa) ASTM C297