EPOCAST 1633

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOCAST 1633

Main features

  • Non-Flowing Cartridge Application
  • Flexible Room-Temperature or Heat Cure
  • Honeycomb Fastener Potting

Product Description

EPOCAST 1633 A/B Epoxy Syntactic is a two-component, halogen-free, self-extinguishing medium-paste compound for potting fasteners in honeycomb structures. The system is non-flowing and cartridge-capable, supporting controlled placement in localized potting areas. Part A and Part B mix at 100:50 by weight and may be cured for three days at room temperature or with shorter elevated-temperature schedules after room-temperature gel. Typical cured compressive strength is 6,500 psi, with 1,400 psi tensile lap shear under the stated conditions.

Key features

  • Non-flowing cartridge application: The medium-paste system is cartridge-capable and remains in place after dispensing.
  • Flexible cure schedules: The system supports room-temperature cure or shorter elevated-temperature cycles after gel.
  • Cured mechanical strength: Typical cured compressive strength is 6,500 psi with 1,400 psi tensile lap shear.

Applications

  • Potting fasteners in honeycomb structures

Technical Specifications

General Properties
Color
The color
White
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
2-5 minutes
Physical Properties
Viscosity (Part B)
soft-paste mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received and storage data for the two-component system.

Property Value Unit Method / condition
Appearance Medium paste - As supplied
Flow behavior Non-flowing - As supplied
Mix ratio by weight 100:50 - Part A:Part B
Storage temperature 60 to 90 deg F Original sealed containers
Shelf life 12 months Under the stated storage conditions
Application format Cartridge-capable - Medium-paste system
Technical properties

After-processing / final-state properties

Typical cured properties and cure options for EPOCAST 1633 A/B.

Property Value Unit Method / condition
Cure schedule 3 days at room temperature; or room-temperature gel plus 5 h at 49 deg C; or 2 h at 66 deg C - Typical cure options
Compressive strength 6,500 psi Typical cured material
Tensile lap shear 1,400 psi Typical cured material
Flammability Self-extinguishing - Cured epoxy syntactic