EPOCAST 1511

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1511

Main features

  • Non-Sag Placement Control
  • 40 to 60-Minute Working Window
  • BMS 5 to 28 Type 3 Qualified

Product Description

EPOCAST® 1511 A/B is a high-density, non-flowing, two-part epoxy syntactic paste for edge filling honeycomb structures and metal fairings, as well as for bonding applications. The gray mixed system uses a 100:15 resin-to-hardener ratio by weight and provides a typical 40–60 minute work life for a 50 g mass at 25°C. It can cure for 24 hours at room temperature or be gelled at room temperature and post-cured for 5 hours at 52°C. After cure, typical properties at 25°C include 69 MPa compressive strength and 310 MPa compressive modulus. EPOCAST® 1511 A/B is qualified to BMS 5-28, Type 3.

Key features

  • Non-flow edge filler: Paste consistency supports controlled placement in honeycomb edges and metal fairings.
  • Practical processing window: Provides a typical 40–60 minute work life for a 50 g mass at 25°C.
  • Flexible cure options: Supports a 24-hour room-temperature cure or an accelerated 5-hour cure at 52°C after gelling at room temperature.

Applications / Suitable for

  • Honeycomb structure edge filling
  • Metal fairing edge filling
  • Bonding applications requiring a non-flowing epoxy syntactic paste

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray
Density (g)
1.25 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:15
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
195000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-system and processing data. Values are typical and are not product specifications.

Property Value Unit Method / condition
Appearance Resin: gray; Hardener: off-white; Mixed system: gray — Visual
Density Resin: 1.20; Hardener: 1.15; Mixed system: 1.25 g/cm³ ASTM D1622; typical at 25°C
Viscosity / consistency Resin: 195,000; Hardener: paste; Mixed system: paste cP / form ASTM D2196; typical at 25°C
Mix ratio 100:15 parts by weight EPOCAST 1511 A Resin:EPOCAST 1511 B Hardener
Material temperature before mixing Above 18 °C Mix both components thoroughly for several minutes
Work life 40–60 min Typical; 50 g mixed mass at 25°C
Typical cure cycle 24 h at room temperature; or gel at room temperature plus 5 h at 52°C — Typical processing cycle
Maximum flow 2.5 (6.4) in (cm) Typical; BMS 5-28
Technical properties

After-processing / final-state properties

Typical cured-material and bonded-joint data under the stated test conditions. Values are not guaranteed design specifications.

Property Value Unit Method / condition
Tensile lap shear 1,200 (8.3) psi (MPa) ASTM D1002; chromic-acid-etched aluminum
Compressive strength 10.0 (69) ksi (MPa) ASTM D695; typical at 25°C
Compressive modulus 45 (310) ksi (MPa) ASTM D695; typical at 25°C
Weight gain after immersion 1.0 in each listed medium % ASTM D543; 24 h at 25°C in TT-S-735 Type III test fluid, MIL-H-5606 hydraulic fluid, Skydrol 500-A and distilled water