EPIBOND 8543

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPIBOND 8543

Main features

  • Fast Setting Epoxy Bonding
  • 1:1 Controlled Mixing
  • Paste Consistency for Bonding

Product Description

Epibond® 8543 C/B Epoxy Adhesive is a two-part, fast-setting epoxy adhesive designed for rapid repair and bonding applications, including use at lower temperatures. The system features a convenient 1:1 mix ratio and paste consistency for controlled application. At 77°F (25°C), bonded assemblies may be handled in approximately 10 minutes and develop high strength within one hour. The contrasting white resin and black hardener produce a uniform gray color when fully mixed, providing visual confirmation of proper mixing. Epibond® 8543 C/B is qualified to BMS 5-123 Type 1 Class 3 and is supplied in cartridge and bulk formats for industrial bonding and repair operations.

Key features

  • Fast-setting epoxy system: Bonded parts may be handled in approximately 10 minutes at 77°F (25°C), supporting rapid repair and assembly operations.
  • 1:1 mix ratio: Equal-part mixing by weight or volume simplifies dispensing and preparation.
  • Visual mix verification: Contrasting component colors produce a uniform gray adhesive after complete mixing.

Applications / Suitable for

  • Quick repair and bonding applications
  • General industrial assembly operations
  • Bonding applications requiring rapid strength development
  • Repair work at ambient and cooler operating temperatures

Technical Specifications

General Properties
Color
The color
Gray
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Resin / Hardener)
Density (g)
1.25 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of Epibond® 8543 C/B components and mixed adhesive prior to cure.

Property Value Unit Method / condition
Mix Ratio 1:1 By volume Resin to hardener
Density 1.25 g/cc Mixed system, ASTM D1875, 77°F (25°C)
Viscosity Paste — Mixed system, ASTM D2196, 77°F (25°C)
Gel Time 3 min 20 g mass, ASTM D2471, 77°F (25°C)
Shelf Life 1 year Stored at +2°C to +40°C in original sealed container
Technical properties

After-processing / final-state properties

Typical cured adhesive properties. Values are typical results and are not specifications.

Property Value Unit Method / condition
Tensile Lap Shear Strength 2100 psi ASTM D1002, Al-Al, -67°F (-55°C)
Tensile Lap Shear Strength 2000 psi ASTM D1002, Al-Al, 77°F (25°C)
Tensile Lap Shear Strength 500 psi ASTM D1002, Al-Al, 180°F (83°C)
Standard Cure 30-60 min 77°F (25°C)