EPIBOND 1534

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPIBOND 1534

Main features

  • 2-Hour Work Life
  • High-Strength Aluminum Bonding
  • BMS 5-126 Qualification

Product Description

EPIBOND® 1534-A/B Epoxy Adhesive is a two-part epoxy adhesive system developed for bonding fiberglass reinforced plastics, metals, and a variety of other substrates. Qualified to Boeing BMS 5-126 Type 2, Class 1, this adhesive combines a long working life with high bond strength, making it suitable for assembly processes that require extended positioning and handling time. The mixed adhesive provides a 2-hour work life at 25°C and develops strong aluminum-to-aluminum lap shear strength after cure. EPIBOND 1534-A/B also retains useful mechanical properties after exposure to water, fuel, and hydraulic-fluid environments, supporting evaluation for aerospace and industrial bonding applications.

Key features

  • BMS 5-126 qualified: Qualified to Boeing BMS 5-126 Type 2, Class 1 requirements for aerospace adhesive applications.
  • Extended work life: Provides approximately 2 hours of work life at 25°C for mixing, positioning, and assembly operations.
  • High structural bond strength: Achieves typical aluminum-to-aluminum lap shear strength of 3,000 psi (20.7 MPa) at 25°C after cure.

Applications / Suitable for

  • Bonding fiberglass reinforced plastics (FRP).
  • Bonding metal assemblies.
  • Aerospace bonding applications requiring BMS 5-126 qualification.
  • Industrial assemblies requiring extended working time before cure.

Technical Specifications

General Properties
Color
The color
Amber
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two
Density (g)
1.05 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the adhesive components and mixed system prior to cure.

Property Value Unit Method / condition
Mix Ratio 100 : 100 parts by weight 1534-A resin to 1534-B hardener
Density 1.05 g/cc Mixed adhesive, ASTM D792
Viscosity 2,000 cP 25°C, mixed adhesive, ASTM D2196
Work Life 2 hours 100 g mass at 25°C, ASTM D1338
Shelf Life 24 months Unopened containers at 25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive properties. Values are typical test results and not specifications.

Property Value Unit Method / condition
Tensile Lap Shear Strength 3,000 psi Al/Al, 25°C, ASTM D1002
Tensile Lap Shear Strength 3,150 psi Al/Al, -55°C, ASTM D1002
Tensile Lap Shear Strength 575 psi Al/Al, 83°C, ASTM D1002
Lap Shear After JP-4 Immersion 2,300 psi 7 days at 25°C, ASTM D543
Lap Shear After Hydraulic Fluid Exposure 2,500 psi TT-S-735 Type III test fluid