EPIBOND 1210

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

EPIBOND 1210

Main features

  • Low-Outgassing Epoxy Bonding
  • 50 to 75-Minute Working Window
  • Flexible Cured Adhesive

Product Description

EPIBOND® 1210 A-1/B Epoxy Adhesive is a two-part, tan epoxy adhesive with a semi-paste consistency and low-outgassing performance for spacecraft bonding applications. The 100:65 parts-by-weight mix provides a 50–75 minute work life at 25°C and cures either for 48 hours at 23–26°C or for 2 hours at 66°C. The system can be applied by brush, spatula, or automatic dispensing equipment. EPIBOND® 1210 B hardener may be increased to as much as 100 parts by weight per 100 parts resin when a more flexible bondline is required. The adhesive is intended for bonding metals, wood and wood products, glass, ceramics, most plastics, and other materials.

Key features

  • Low-outgassing performance: Typical ASTM E595 results are 0.65% total mass loss and 0.01% collected volatile condensable material.
  • Adjustable bondline flexibility: The hardener level may be increased from 65 to as much as 100 parts by weight per 100 parts resin for more flexible bonds.
  • Flexible cure options: Cures at room temperature in 48 hours or with an accelerated 2-hour cure at 66°C.

Applications / Suitable for

  • Spacecraft bonding applications
  • Metal bonding
  • Wood and wood-product bonding
  • Glass and ceramic bonding
  • Bonding most plastics

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Tan / Tan
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Resin/ Hardener)
Density (g)
1.5 / 1.0 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values at 25°C unless otherwise stated. These values do not constitute a product specification.

Property Value Unit Method / condition
Density at 25°C 1.5 / 1.00 / 1.30 g/cm³ ASTM D792; A-1 resin / B hardener / mixed system
Viscosity at 25°C 250,000 / 30,000 / semi-paste cP / cP / — ASTM D2393; A-1 resin / B hardener / mixed system
Solids 100 % ASTM D1644; mixed system
Mix ratio 100:65 Parts by weight EPIBOND® 1210 A-1 resin : EPIBOND® 1210 B hardener
Work life 50–75 min 100 g mixed mass at 25°C
Typical cure cycles 48 h at 23–26°C; 2 h at 66°C — Typical room-temperature or accelerated cure options
Storage temperature 2–40 °C Dry place in original sealed containers; protect from direct sunlight
Shelf life 1 year From date of shipment under the specified storage conditions
Technical properties

After-processing / final-state properties

Typical cured-system and bonded-joint values. Results depend on the stated substrate, temperature, exposure, and test method and do not constitute guaranteed specifications.

Property Value Unit Method / condition
Maximum service temperature 200 (93) °F (°C) ASTM D648
Tensile lap shear 2,500 (17.2) / 2,500 (17.2) psi (MPa) ASTM D1002; aluminum-to-aluminum / steel-to-steel at 25°C
Tensile lap shear 500 (3.4) psi (MPa) ASTM D1002; steel-to-steel at 66°C
Tensile lap shear 1,800 (12.4) psi (MPa) ASTM D1002; polyester-to-polyester at 25°C
Lap shear after fluid immersion 2,550 (17.5) / 2,600 (17.9) / 2,700 (18.6) psi (MPa) ASTM D1002; 7 days at 23°C in JP-4 / Skydrol / distilled water
Coefficient of thermal expansion α1: 76.6; α2: 216.7 ppm/°C Cured material
Thermal conductivity 0.41 W/mK Cured material
Outgassing TML: 0.65 / CVCM: 0.01 % ASTM E595; total mass loss / collected volatile condensable material