ENTHONE B3

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE B3

Main features

  • Four-Hour Ink Pot Life
  • Controlled Heat-Cure Processing
  • Faster Cure at Higher Temperature

Product Description

ENTHONE B-3 Catalyst is a heat-cure-only catalyst component for ENTHONE M-Series epoxy marking inks. It provides an average 4-hour pot life after the specified induction period, giving a defined processing window before the ink begins to solidify. Cure temperature must exceed 79 deg C, and higher temperatures shorten the required cure time within the published ink-film schedule. B-3 is used where permanent epoxy markings are processed through controlled thermal cure, including supported M-Series color packages and premeasured bi-pack configurations.

Key features

  • Heat-Cure-Only Processing: B-3 is used exclusively with controlled thermal cure.
  • Four-Hour Pot Life: The catalyzed ink has an average 4-hour working pot life after induction.
  • Temperature-Responsive Cure: Higher cure temperatures reduce the required ink-film cure time.

Applications / Suitable for

  • ENTHONE M-Series heat-cured marking inks
  • M 0 N and M 9 N bi-pack configurations
  • M 0 NC nonconductive black bi-pack configurations

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber Liquid
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
160 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
73.889 °C
Physical Properties
VOC
720 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

Typical catalyst and catalyzed-ink processing data. Final properties belong to the selected M-Series ink, catalyst ratio, and cure schedule.

Property Value Unit Method / condition
Catalyst function Basic heat-cure catalyst - ENTHONE M-Series epoxy marking inks
Cure mode Heat only - B-3 catalyst
Average pot life 4 hr Begins after induction period
Induction period 30 min All standard catalysts, including B-3
Required cure temperature >79 deg C Above 175 deg F
Shelf life 2 years All ENTHONE catalysts; from date of manufacture