ENTHONE B13/28

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE B13/28

Main features

  • Accelerated Three-Day Ambient Cure
  • One-Hour Processing Window
  • Nonconductive Black Ink Compatibility

Product Description

ENTHONE B-13/28 Catalyst is an accelerated ambient-cure catalyst option for ENTHONE M-Series and 50-Series epoxy marking inks. The catalyzed ink reaches room-temperature cure in approximately 3 days and has an average 1-hour pot life after the induction period. A tack-free surface develops in about 1 to 1.5 hours, although this stage is not full cure. B-13/28 may also be heat cured and is the recommended catalyst for M 0 NC and 50 770R nonconductive black inks, providing a defined process route for permanent electronic marking.

Key features

  • Accelerated Ambient Cure: Room-temperature cure is completed in approximately 3 days.
  • One-Hour Pot Life: The catalyzed ink has an average 1-hour processing window after induction.
  • Nonconductive Black Ink Match: B-13/28 is recommended for M 0 NC and 50 770R nonconductive black inks.

Applications / Suitable for

  • ENTHONE M-Series epoxy marking inks
  • ENTHONE 50-Series epoxy marking inks
  • M 0 NC and 50 770R nonconductive black inks

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear Liquid
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
68.33 °C
Physical Properties
VOC
930 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

Typical catalyst and catalyzed-ink processing data. Final properties belong to the selected ink color, catalyst ratio, and cure schedule.

Property Value Unit Method / condition
Catalyst function Accelerated ambient cure - ENTHONE M-Series and 50-Series inks
Cure mode Room temperature or heat - Catalyst B-13/28
Room-temperature cure 3 days Catalyzed ink system
Average pot life 1 hr Begins after induction period
Tack-free time 1 to 1.5 hr Depends on ink-film thickness; not full cure
Recommended inks M 0 NC; 50 770R - Nonconductive black ink variants

Leading Brands Trust in Our Products and Services