ENTHONE AD3002

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE AD3002

Main features

  • Two to Four Percent Flow Adjustment
  • Crawling and Pinholing Control
  • Gentle Post-Induction Mixing

Product Description

ENTHONE AD3002 Flow Agent is a process additive for ENTHONE M-Series and 50-Series epoxy marking inks. It adjusts ink flow where crawling, pinholing, or bubbling affects printed-film appearance. The recommended addition is 2 to 4% by weight, introduced after the catalyst induction period so the additive does not interfere with catalyzation. Gentle mixing is specified to avoid overmixing. AD3002 is selected for controlled flow correction within the matched ENTHONE ink system rather than as a standalone coating material.

Key features

  • Two to Four Percent Adjustment: A 2 to 4% by-weight addition provides targeted flow correction.
  • Post-Induction Addition: The flow agent is introduced after the catalyst induction period.
  • Controlled Gentle Mixing: Gentle mixing limits overmixing while addressing crawling, pinholing, and bubbling.

Applications / Suitable for

  • ENTHONE M-Series flow adjustment
  • ENTHONE 50-Series flow adjustment
  • Printed legend and marking film flow correction
Product Family

ENTHONE AD3002

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Clear

Additional Information

Technical properties

As-supplied / before-processing properties

Processing data for AD3002 used with catalyzed ENTHONE marking inks. The additive does not have a separate cured final state.

Property Value Unit Method / condition
Primary function Flow adjustment - ENTHONE M-Series and 50-Series marking inks
Recommended addition 2 to 4 wt% Add incrementally
Addition timing After induction period - Prevents interference with catalyzation
Mixing method Gentle mixing - Avoid overmixing
Targeted flow conditions Crawling, pinholing, bubbling - Printed ink-film application