ENTHONE AD2002

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ENTHONE AD2002

Main features

  • Spray-Application Viscosity Control
  • Air-Pressure and Orifice Adjustment
  • Extended Catalyzed-Ink Pot Life

Product Description

ENTHONE AD2002 Thinner is a process additive used to prepare ENTHONE M-Series and 50-Series epoxy marking inks for spray application. It is added after the catalyst induction period, with the amount adjusted to spray-unit air pressure and orifice. The M-Series guide specifies 25 to 40% by volume; the 50-Series guide allows 25 to 50% by volume. AD2002 extends the catalyzed ink pot life considerably and may also be used for localized equipment cleaning before the ink dries or partially cures.

Key features

  • Spray-Application Thinning: AD2002 adjusts catalyzed ENTHONE inks for spray equipment and atomization conditions.
  • Ink-Specific Addition Ranges: Addition is 25 to 40% by volume for M-Series and 25 to 50% for 50-Series.
  • Extended Pot Life: Thinner addition substantially lengthens the catalyzed ink working period.

Applications / Suitable for

  • ENTHONE M-Series spray application
  • ENTHONE 50-Series spray application
  • Localized marking-equipment cleaning before partial cure

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear Liquid
Vapor Density
>1 (Air =1)
Vapor Pressure
16 mmHg
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
115.5 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
21.111 °C
Physical Properties
VOC
910 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and spray-processing data for AD2002. Addition ranges depend on the selected ENTHONE ink family and spray equipment.

Property Value Unit Method / condition
Physical state Liquid - As supplied
M-Series addition 25 to 40 vol% After induction; adjust for spray air pressure and orifice
50-Series addition 25 to 50 vol% After induction; adjust for spray air pressure and orifice
Relative density 0.901 - As-supplied measurement
Storage temperature 5 to 40 deg C As-supplied condition