ENTHONE AD2001

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ENTHONE AD2001

Main features

  • Incremental 3 to 6% Thinning
  • Post-Induction Process Control
  • Extended Ink Pot Life

Product Description

ENTHONE AD2001 Thinner is a process additive for nominal viscosity adjustment of ENTHONE M-Series and 50-Series epoxy marking inks. It is introduced in small increments after the required catalyst induction period, normally at 3 to 6% by weight. The thinner extends the working pot life of the catalyzed ink and is also listed for localized equipment cleaning before ink dries or partially cures. AD2001 provides controlled viscosity reduction for screen-printing and other marking processes while remaining within the matched ENTHONE ink system.

Key features

  • Incremental Viscosity Adjustment: A 3 to 6% by-weight addition provides controlled nominal viscosity reduction.
  • Post-Induction Addition: AD2001 is added only after the catalyst induction period.
  • Pot-Life Extension: Thinner addition extends the working pot life of catalyzed ENTHONE ink.

Applications / Suitable for

  • ENTHONE M-Series viscosity adjustment
  • ENTHONE 50-Series viscosity adjustment
  • Localized marking-equipment cleaning before partial cure

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear Liquid
Density
Volumetric mass per unit
0.979 kg/m3
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
182.22 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
57.23 °C
Physical Properties
VOC
979 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

Processing data for AD2001 used with catalyzed ENTHONE marking inks. The additive does not have a separate cured final state.

Property Value Unit Method / condition
Primary function Nominal viscosity adjustment - ENTHONE M-Series and 50-Series marking inks
Recommended addition 3 to 6 wt% Add incrementally
Addition timing After induction period - Add after ink and catalyst have completed induction
Process effect Extends pot life - Applies to the catalyzed ink mixture