ENTHONE 50 Series

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ENTHONE 50

Main features

  • Ambient or Heat-Cure Flexibility
  • Multi-Method Permanent Marking
  • Chemical- and Thermal-Resistant Films

Product Description

ENTHONE 50-Series Inks are permanent, two-component epoxy screen-printing inks for durable legend and component marking. The family adheres to photoimageable, thermal, and UV solder masks as well as glass, metal, and compatible plastics when properly applied and cured. Catalyst options provide room-temperature or heat-cure processing, while screen printing, spraying, brushing, and roller printing support several marking methods. Cured films provide chemical and thermal resistance, with color-specific electrical insulation data defined for controlled cure and humidity conditions. Applications include circuit boards, semiconductor components, connectors, dials, nameplates, chassis, glass, and thermoplastics.

Key features

  • Multiple Marking Methods: Screen printing, spraying, brushing, and roller printing cover varied production requirements.
  • Flexible Catalyst Cure: Available catalyst options support room-temperature or controlled heat cure.
  • Cured Electrical Characterization: Color-specific insulation resistance is defined before and after humidity conditioning.

Applications / Suitable for

  • Permanent circuit-board legends
  • Semiconductor-component marking
  • Connectors, dials, and nameplates
  • Chassis and edge-lit panels
  • Glass and thermoplastic marking

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Ink / Catalyst)

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing data for the ENTHONE 50-Series family. Color- and catalyst-specific conditions are identified where applicable.

Property Value Unit Method / condition
Standard catalyst addition 4.0 to 9.0 parts by weight Per 100 parts ink; exact value depends on 50-Series color and catalyst
Catalyst 5 addition 7.0 to 11.5 parts by weight Per 100 parts ink; only for colors where Catalyst 5 is recommended
Induction period 30; 60 min All standard catalysts; Catalyst 5, respectively
Average pot life 1 to 24 max hr Depends on selected catalyst; measured after induction
Shelf life Ink 3; catalysts 2 years From date of manufacture
Screen mesh 180 to 350 mesh count Monofilament polyester, metallized polyester, or equivalent stainless steel
Squeegee hardness 60 to 80 durometer Sharp, nick-free squeegee for screen printing
Technical properties

After-processing / final-state properties

Typical cured-film data for specified colors and cure conditions. Electrical values vary by ink color and cure schedule.

Property Value Unit Method / condition
Recommended cured film thickness 0.7 to 1.4 (0.017 to 0.035) mil (mm) Cured ink film
Initial insulation resistance 50 700R: 1.4 x 10^8; 50 710R: 1.2 x 10^4; 50 770R, 50 771R, and all other colors: >1.0 x 10^12 ohm MIL-I-43553A; cured 30 min at 121 deg C
Insulation resistance after humidity 50 700R: 1.7 x 10^8; 50 710R: 1.2 x 10^4; 50 770R, 50 771R, and all other colors: >1.0 x 10^10 ohm MIL-I-43553A; 77 +/- 10 deg F and 95% RH for 48 hr; cured 30 min at 121 deg C
Low-outgassing cure condition 30 at 150 min at deg C Extended cure for low-outgassing properties

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers