ELANTAS TU-956

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS TU-956

Main features

  • Two-Part Elastomer Casting
  • Defined Mixed-Material Processing
  • Mechanical and Dielectric Characterization

Product Description

CONATHANE TU-956 Two-Component Urethane Casting System is a two-component urethane casting system in the TU-950 series for forming cured elastomer parts. The product is processed as a mixed liquid system with defined mixed viscosity, pot life, and cure behavior. Its cured material is characterized by hardness, tensile strength, elongation, dielectric strength, and volume resistivity, combining mechanical and electrical selection data within one casting grade. TU-956 is suited to controlled elastomer-casting evaluations where both physical response and dielectric behavior must be considered.

Key features

  • Two-Part Casting Process: Separate components are mixed before the liquid urethane is cast and cured.
  • Defined Processing Window: The product is characterized by mixed viscosity, pot life, and cure behavior.
  • Mechanical and Electrical Profile: Cured characterization includes hardness, strength, elongation, dielectric strength, and resistivity.
Product Family

ELANTAS TU-956

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
translucent
Color
The color
amber
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.09
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
24 kV/mm
Surface Resistivity
6.10 x 10^13 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
5.9 x 10^12 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing and material properties before cure.

Property Value Unit Method / condition
Mix Ratio (A/B) 100/28 Weight Part A to Part B
Initial Mixed Viscosity 5,000 cP Initial mixed material
Pot Life 8 min 25°C
Demold Time 16 hr 25°C
Appearance Translucent Amber — Typical appearance
Technical properties

After-processing / final-state properties

Typical cured properties of CONATHANE® TU-956.

Property Value Unit Method / condition
Hardness 55 Shore D Typical cured value
Tensile Strength 5,400 psi Typical cured value
Elongation 400 % Typical cured value
Tear Strength (Die C) 615 pli Die C
Heat Distortion Temperature 104 °C Elevated cure