ELANTAS S-13

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ELANTAS S-13

Main features

  • Dedicated Resin-Reduction Function
  • Single-Product Solvent Blend
  • Controlled Formulation Adjustment

Product Description

CONAP S-13 Solvent is a solvent blend used as a resin reducer in compatible industrial resin-processing operations. The product is a nonreactive liquid adjustment material rather than an adhesive, coating, encapsulant, or cured resin. Its dedicated S-13 formulation supports controlled reduction of the host resin before application or processing. CONAP S-13 is suited to operations that specifically require this reducer and where the solvent addition, handling method, and acceptable resin adjustment are established by the applicable process instructions.

Key features

  • Resin-Reduction Function: S-13 is used to reduce compatible resin systems before processing.
  • Dedicated Solvent Blend: The product is supplied as a nonreactive liquid reducer rather than a curable resin.
  • Process-Specific Use: Application depends on the host resin and the controlled reduction procedure.
Product Family

ELANTAS S-13

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
water-white
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.85-0.88
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CONAP® S-13 as supplied. Values are typical and not intended as specifications.

Property Value Unit Method / condition
Color Water-white — 25°C (77°F)
Specific Gravity 0.85-0.88 — 20°C (68°F)
Flash Point 27 °C Closed Cup
Density 0.87 g/cm³ 25°C (77°F)
Viscosity, Kinematic <19 mm²/s 40°C (104°F)