LAIRD ECCOSHIELD VY

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD ECCOSHIELD VY

Main features

  • Non-Hardening Conductive RF-Seam Compound
  • 0.001 ohm-cm Volume Resistivity
  • 40 to 288 deg C Service Range

Product Description

ECCOSHIELD® VY Conductive Caulking Compound is a single-component, metallic-particle-filled, electrically conductive sealer for radio-frequency-shielded structures. The non-hardening compound is applied with conventional caulking equipment to fill and seal seams, joints, cabinet interfaces, conduit connections, and threaded areas requiring electrical continuity. It remains pliable after application and is documented for structures exposed to vibration, temperature change, or joint displacement. Typical data include 0.001 ohm·cm volume resistivity, service from -40°C to 288°C, and insertion loss greater than 100 dB at a caulked joint.

Key features

  • Non-hardening conductive seal: The single-component caulking compound remains pliable after application.
  • Low volume resistivity: Typical volume resistivity is 0.001 ohm·cm.
  • RF shielding performance: Documented insertion loss is greater than 100 dB at a caulked joint.

Applications / Suitable for

  • Radio-frequency-shielded cabinets and structures
  • Seams, joints, conduit connections, and threads
  • Removable covers requiring conductive sealing

Technical Specifications

General Properties
Color
The color
Silver / Grey
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
4.9 / 2.05
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
>100 / 50-60 Ohms⋅cm
Thermal Properties
Service temperature
-40 to +280 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Single-component non-hardening caulking compound N/A As supplied
Density 4.9 g/cm³ As supplied
Bead yield 33.5 m/kg 3 mm diameter bead
Minimum application temperature 20 °C Recommended application condition

Technical properties

After-processing / final-state properties

Typical final-state values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Volume resistivity 0.001 ohm·cm Typical applied material
Service temperature range -40 to 288 °C Documented operating range
Insertion loss >100 dB Measured at a caulked joint