ECCOBOND LUX OGR146TUV

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

ECCOBOND LUX OGR146TUV

Main features

  • UV and Shadow-Area Thermal Cure
  • Low-Refractive-Index Optical Bonding
  • Extended 91-Day Working Window

Product Description

LOCTITE ECCOBOND LUX OGR146TUV is a one-part photocurable acrylate adhesive for optical devices, fiber-optic assemblies, and optoelectronic components. UV exposure provides the primary cure, and secondary thermal schedules of 1 hour at 100 deg C or 2 hours at 85 deg C address material in shadowed areas after light curing. The cured adhesive has a low refractive index across multiple optical wavelengths, including 1.464 at 589 nm and 1.454 at 1550 nm. A 91-day work life at 25 deg C supports extended process availability for controlled, high-throughput assembly.

Key features

  • UV and Thermal Dual Cure: UV cure is supplemented by defined thermal schedules for adhesive in shadowed areas.
  • Low Refractive Index: Cured refractive index ranges from 1.464 at 589 nm to 1.454 at 1550 nm.
  • Extended Work Life: A 91-day work life at 25 deg C supports long process availability before cure.

Applications / Suitable for

  • Optical devices
  • Fiber-optic assembly
  • Optoelectronic assembly
  • High-throughput optical assembly

Technical Specifications

General Properties
Color
The color
Colorless
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,250 mPa.s
Other Properties
Storage Temperature
-5 to +5 °C
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
77 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical class Acrylate - As supplied
Component count One-part - As supplied
Work life 91 days At 25 deg C
Primary cure wavelength 365 nm UV light
Secondary thermal cure 1 hour at 100 deg C or 2 hours at 85 deg C - After light cure for shadowed areas
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Refractive index 1.464 - At 589 nm
Refractive index 1.458 - At 830 nm
Refractive index 1.454 - At 1550 nm
Tensile modulus 635 N/mm^2 DMTA at 25 deg C
Moisture absorption at saturation 1.7 wt.% 85 deg C and 85% RH