ECCOBOND FP0066

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ECCOBOND FP0066

Main features

  • Conductive Semiconductor Encapsulation
  • Two-Hour Cure at 60 deg C
  • Firm Shore D 80 Cure

Product Description

LOCTITE ECCOBOND FP0066 is a single-component, gray, heat-cure conductive epoxy encapsulant for semiconductor applications. The liquid formulation combines electrical conductivity with a hard cured profile for protecting and fixing semiconductor features where a conductive encapsulation material is required. An alternate cure of 2 hours at 60 deg C supports controlled thermal processing, while storage at -40 deg C provides a 30-day shelf-life basis for material planning. The cured epoxy reaches Shore D 80 and a typical bulk volume resistivity of 0.02 ohm cm; the values apply to the stated cure and test conditions.

Key features

  • Conductive Epoxy Encapsulation: A typical bulk volume resistivity of 0.02 ohm cm supports conductive semiconductor encapsulation after cure.
  • Controlled Heat Cure: An alternate 2-hour cure at 60 deg C provides a defined thermal-processing option.
  • Hard Cured Profile: Typical Shore D 80 hardness provides a firm final encapsulant state.

Applications / Suitable for

  • Semiconductor encapsulation
Product Family

ECCOBOND FP0066

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray liquid
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.02 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Technology Epoxy - As supplied
Appearance Gray liquid - As supplied
Cure mechanism Heat cure - Processing classification
Shelf life 30 days Stored at -40 deg C
Alternate cure schedule 2 hours At 60 deg C