DYMAX 910

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 910

Main features

  • Light-Activated Localized Tacking
  • Targeted PCB Wire Strain Relief
  • Organized Wire Unitization

Product Description

Dymax Light Weld 910 Adhesive for Wire and Parts Tacking is a single-component light-curable adhesive for securing wires and small parts on printed circuit boards. After wires or components are positioned, localized light exposure cures the material at the tack point. The adhesive is suited to wire and parts tacking, strain relief, and wire unitization, helping organize routed conductors and reinforce selected attachment points. Its focused dispense-and-cure approach supports discrete assembly work without coating or encapsulating the surrounding board area.

Key features

  • Localized Light-Cure Tacking: Light activation secures wires or small parts after positioning on the board.
  • PCB Wire Strain Relief: Applied around routed wires to reinforce localized stress points.
  • Wire Unitization: Joins wire groups into a more organized assembly for downstream handling.

Applications / Suitable for

  • Wire tacking on printed circuit boards
  • Parts tacking on printed circuit boards
  • Strain relief
  • Wire unitization
Product Family

DYMAX 910

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light Straw
Chemistry Type
Urethane (Meth)Acrylate
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
12.7 mm
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
95 °C
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for Dymax Light Weld® 910 UV-curable wire and parts tacking adhesive.

Property Value Unit Method / condition
Chemical Class Urethane (Meth)Acrylate - As supplied
Appearance Light Straw - Visual
Solvent Content 100 % solids Contains no solvent
Flash Point >200 °F Typical value
Viscosity Non-flowing Thixotropic Paste - Dispensing state
Time to Full Cure <5 seconds 1/16" bead, >100 mW/cm² UV intensity
Technical properties

After-processing / final-state properties

Typical cured properties for Dymax Light Weld® 910 adhesive after UV exposure.

Property Value Unit Method / condition
Durometer Hardness A60 Shore A UV cured
UV Cured Film Thickness 0.5 in Maximum cured thickness
Tensile Strength 500 psi Glass-to-steel
Thermal Limit (Brittle/Degrades) -50 / 300 °F Cured adhesive
Dielectric Strength 500 V/mil Electrical property
Dielectric Constant @ 1 MHz 3.27 - 1 MHz test frequency
Surface Resistivity 60 ×10¹² Ω Electrical property

Leading Brands Trust in Our Products and Services