DYMAX 846-GEL

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 846-GEL

Main features

  • Activator-Managed Fast Fixturing
  • High-Shear Structural Bonding
  • Thermal-Shock-Resistant Bonded Assemblies

Product Description

Dymax 846-GEL Structural Adhesive is a high-strength structural adhesive gel that cures through contact with specified Dymax activators, including 535-A-REV-A and 501-E-REV-A. The gel form supports controlled placement before assembly, while activator selection and application govern fixture development and final bond performance. Product data support high tensile-shear strength and thermal-shock resistance within the tested substrate and cure configurations. Applications include bonding ferrite magnets in DC motor assemblies, joining dissimilar substrates, and bonding metal frames where the activator, surface preparation, bondline, and service conditions are appropriate.

Key features

  • Activator-controlled cure: Specified Dymax activators initiate fixture and final bond development.
  • High tensile-shear performance: The cured adhesive is positioned for structural joints within the tested configurations.
  • Thermal-shock resistance: The bonded assembly is documented for thermal-shock exposure under product-specific conditions.

Applications / Suitable for

  • Ferrite magnet bonding in DC motor assemblies
  • Joining dissimilar substrates
  • Metal frame bonding

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent Straw
Density (g)
1.06 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
29,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Application and cure-system characteristics before structural bond development.

Property Value Unit Method / condition
Physical form Structural adhesive gel As supplied
Application behavior Controlled gel placement Before assembly
Cure initiation Dymax activator Activator-dependent cure
Compatible activators 535-A-REV-A; 501-E-REV-A Activator options
Process boundary Activator and surface preparation required Before fixture and final cure
Technical properties

After-processing / final-state properties

Bonded-state characteristics within the specified activator, substrate, and test conditions.

Property Value Unit Method / condition
Fixture development Activator-dependent Timing varies with activator and assembly conditions
Tensile-shear performance High Within the stated test configuration
Thermal-shock behavior Resistant Within the stated exposure scope
Structural bond scope Ferrite magnets; dissimilar substrates; metal frames Applications
Final performance boundary Substrate- and cure-specific Do not generalize beyond tested configurations