DYMAX 730-BT

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 730-BT

Main features

  • Visible Blue Mask Placement
  • Acid-and-Alkali Process Resistance
  • Peelable Post-Process Removal

Product Description

Dymax SpeedMask 730-BT Maskant is a blue peelable UV/visible-light-curable process maskant for temporary protection in harsh chemical and abrasive operations. The gel format supports controlled placement before cure, and the cured mask is stated for resistance to acid and alkali process exposure within defined limits. After processing, the barrier can be peeled away to restore access to the protected surface. Applications include plating, anodizing, grit or sand blasting, and chemical milling or etching where the exact process conditions match the product data.

Key features

  • Blue coverage visibility: The blue gel provides clear visual contrast for controlled mask placement.
  • Acid-and-alkali resistance: The cured barrier is documented for harsh chemical-process exposure within stated limits.
  • Peelable cleanup: The temporary mask can be peeled from the protected surface after processing.

Applications / Suitable for

  • Plating and anodizing
  • Grit and sand blasting
  • Chemical milling and etching within documented limits

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Blue Translucent Gel
Density (g)
0.96 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
300 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
22,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product characteristics before cure and chemical or abrasive processing.

Property Value Unit Method / condition
Physical form Peelable gel maskant As supplied
Color Blue Before cure
Cure activation UV and visible light Applied maskant
Application behavior Localized gel placement Before cure
Process role Temporary chemical and abrasive protection Before the Stated operations
Technical properties

After-processing / final-state properties

Cured-mask behavior within the stated chemical and removal boundaries.

Property Value Unit Method / condition
Chemical resistance scope Acid and alkali process exposure Within stated process limits
Removal mode Peel removal After processing
Electrochemical process scope Plating; anodizing Stated operations
Material-removal process scope Chemical milling; etching Stated operations
Final application boundary Temporary removable mask Not a permanent coating