DYMAX 717-R

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 717-R

Main features

  • High-Adhesion Process Retention
  • Hot-Water-Assisted Peel Removal
  • Visible Red Mask Placement

Product Description

Dymax SpeedMask 717-R Maskant is a red UV- and visible-light-curable gel maskant for plating, anodizing, aggressive grit blasting, shot peening, machining, and air plasma spray. The product provides high adhesion during process exposure and is removed with a hot-water-assisted peel sequence after use. Its supported application scope also includes protection of orthopedic implants where the exact process and biological-evaluation boundaries are maintained. The gel form supports controlled placement before cure, while the red appearance improves visual identification of masked areas. SpeedMask 717-R is a temporary process-protection material and is not intended to remain as a permanent coating.

Key features

  • Red visual identification: The red gel makes the applied mask area easy to distinguish before and after cure.
  • High-adhesion process hold: The cured mask is intended to remain attached through plating and aggressive mechanical processing.
  • Hot-water-assisted release: The documented removal sequence combines hot water with peel removal after processing.

Applications / Suitable for

  • Plating and anodizing
  • Aggressive grit blasting, shot peening, and machining
  • Air plasma spray and orthopedic implant protection

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Red Translucent Gel
Density (g)
1.10 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
210 %
Chemical Properties
Water Absorption
2.6 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
23,500 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics for placement, identification, and light cure.

Property Value Unit Method / condition
Physical form Gel maskant As supplied
Color Red Before cure
Cure activation UV and visible light Applied maskant
Placement behavior Localized gel application Before cure
Process role Temporary surface protection Before plating, blasting, machining, or spray exposure
Technical properties

After-processing / final-state properties

Cured-mask characteristics, removal, and stated evaluation scope.

Property Value Unit Method / condition
Cured adhesion High During the protected process
Removal method Hot-water-assisted peel After processing
Process exposure scope Plating; anodizing; blasting; peening; machining; plasma spray Stated operations
Biological evaluation scope ISO 10993-5 cytotoxicity evaluation Within the stated test scope
Final application boundary Temporary removable mask Not a permanent coating