DYMAX 711

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 711

Main features

  • Thixotropic Complex-Surface Masking
  • Multi-Metal Blast Protection
  • Peelable Post-Process Removal

Product Description

Dymax SpeedMask 711 Maskant is a thixotropic, light-curable gel maskant for temporary surface protection during grit blasting, shot peening, airflow testing, sand blasting, and mild chemical processing. Its gel rheology supports localized placement on nickel alloys, steel, titanium, stainless steel, and aluminum before UV cure. After processing, the cured mask is designed for peel removal rather than permanent service. The product is suited to metal components that need a defined protective boundary through mechanical or mild chemical exposure, while the thixotropic form helps maintain the applied shape on complex surfaces before cure.

Key features

  • Thixotropic gel definition: The gel form supports localized application and shape retention before cure.
  • Multi-metal process masking: The supported substrate range includes nickel alloys, steels, titanium, and aluminum.
  • Peelable temporary protection: The cured mask can be removed after blasting, peening, testing, or mild chemical exposure.

Applications / Suitable for

  • Grit and sand blasting
  • Shot peening and airflow testing
  • Mild chemical processing
Product Family

DYMAX 711

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless Translucent Gel
Density (g)
1.13 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
200 %
Chemical Properties
Water Absorption
6.9 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
80,000 mPa.s
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Before-processing characteristics for applying the thixotropic maskant to metal surfaces.

Property Value Unit Method / condition
Physical form Thixotropic gel As supplied
Application behavior Localized shape retention Before cure
Cure activation UV light Applied maskant
Metal substrate scope Nickel alloys; steel; titanium; stainless steel; aluminum Application scope
Temporary function Process masking Before mechanical or mild chemical exposure
Technical properties

After-processing / final-state properties

Cured-mask characteristics during process exposure and removal.

Property Value Unit Method / condition
Cured function Temporary protective mask After UV cure
Mechanical process scope Grit blasting; shot peening; sand blasting Stated operations
Test-process scope Airflow testing Stated operation
Chemical process scope Mild chemical processing Stated operation
Removal mode Peel removal After completion of the protected process