DYMAX 6-630-T

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 6-630-T

Main features

  • Glass-to-Metal Structural Bonding
  • Secondary Heat-Cure Completion
  • Fixture and Latch Assembly Fit

Product Description

Dymax Multi-Cure 6-630-T Glass-to-Metal Bonding Adhesive is a structural adhesive developed for glass-to-metal and glass assembly. The material uses UV and visible light for exposed bond areas and includes secondary heat cure for regions that cannot receive sufficient light. Its application scope includes glass fixtures and furniture, automotive latch assemblies, potting, structural glass components, and consumer packaging. The product is differentiated by its focus on glass interfaces, including stated glass-to-stainless steel and glass-to-glass performance evaluation. It suits assemblies that require transparent-substrate light cure together with a secondary route for shadowed sections of the joint.

Key features

  • Glass-interface specialization: The adhesive is positioned for glass-to-metal and glass-to-glass structural assembly.
  • Secondary heat completion: Heat cure can address portions of the bondline outside the effective light path.
  • Fixture and latch applications: Documented uses include glass furniture, structural glass, and automotive latches.

Applications / Suitable for

  • Glass fixtures and furniture
  • Automotive latch assembly
  • Structural glass and consumer packaging
Product Family

DYMAX 6-630-T

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless Translucent Liquid
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.50
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
100 °C
Chemical Properties
Water Absorption
1.5 %

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure characteristics and processing routes for glass-focused structural bonding.

Property Value Unit Method / condition
Product form Structural glass-bonding adhesive As supplied
Primary cure activation UV and visible light Through an appropriate transparent substrate
Secondary cure option Heat Shadowed bondline regions
Primary interface Glass-to-metal Bonding scope
Secondary interface Glass-to-glass Bonding scope
Technical properties

After-processing / final-state properties

Final-state joint scope after light and, where required, secondary heat cure.

Property Value Unit Method / condition
Final function Structural glass-bonded joint After complete cure
Evaluated metal interface Glass-to-stainless steel Performance context
Evaluated glass interface Glass-to-glass Performance context
Assembly applications Fixtures; furniture; automotive latches Within the Application scope
Additional roles Potting; structural glass; consumer packaging Within the Application scope

Leading Brands Trust in Our Products and Services