DYMAX 6-621-GEL

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 6-621-GEL

Main features

  • Controlled Structural Gel Placement
  • Mixed-Material Bonding Coverage
  • Light, Heat, or Activator Cure

Product Description

Dymax Multi-Cure 6-621-GEL Adhesive is a gel-form structural adhesive for metals, glass, ceramic, polyamide, phenolic materials, and other supported substrates. The material cures with UV or visible light in exposed areas and can use secondary heat or a compatible activator where light access is limited. Its gel consistency supports localized placement and retention before cure, making the grade relevant to metal-to-glass bonding, coil winding, potting, and structural battery bonding. The product combines multi-route cure flexibility with a broader mixed-material substrate range for assemblies that include rigid inorganic surfaces and engineering polymers.

Key features

  • Gel-form placement control: The gel consistency supports localized application and bead retention before cure.
  • Mixed-material substrate reach: Supported materials include metals, glass, ceramic, polyamide, and phenolic substrates.
  • Exposed and shadowed cure: Light, heat, and activator pathways support assemblies with varied cure access.

Applications / Suitable for

  • Metal-to-glass bonding
  • Coil winding and potting
  • Structural battery bonding
Product Family

DYMAX 6-621-GEL

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear Translucent Liquid - Gel
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.51
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
79 °C
Chemical Properties
Water Absorption
1.7 %

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and pre-cure characteristics for selecting and placing the gel adhesive.

Property Value Unit Method / condition
Physical form Gel adhesive As supplied
Primary cure activation UV and visible light Exposed adhesive areas
Secondary cure option Heat Areas with limited light access
Activator cure option Compatible activator Close-fitting or shadowed joints
Supported substrate scope Metal; glass; ceramic; polyamide; phenolic Within the Bonding scope
Technical properties

After-processing / final-state properties

Cured-joint characteristics and supported final assembly roles.

Property Value Unit Method / condition
Final function Structural bonded joint After complete cure
Joint placement character Localized gel bondline After cure of the placed gel
Inorganic substrate scope Metal; glass; ceramic Bonded-material scope
Polymer substrate scope Polyamide; phenolic Bonded-material scope
Assembly applications Coil winding; potting; structural battery bonding Within the Application scope

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers