DYMAX 535-A-REV-A

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DYMAX 535-A-REV-A

Main features

  • Close-Gap Multi-Cure Activation
  • Shadowed-Area Bond Processing
  • Metal, Ferrite, and Ceramic Activation

Product Description

Dymax 535-A-REV-A Activator is an amber-brown, isopropyl-alcohol-based activator for Dymax Multi-Cure structural adhesives. Applied as a surface treatment, it initiates or accelerates cure in close-gap joints where direct light exposure may be limited. The activator is used with compatible Dymax adhesives on metals, ferrite, ceramic, glass, and thermoset plastics within the stated gap and application limits. It is a processing component rather than a stand-alone adhesive, so bond performance is established by the selected Multi-Cure adhesive and complete activation procedure. Applications include close-fitting structural joints and assemblies with shadowed bond areas.

Key features

  • Close-gap cure activation: Initiates or accelerates compatible Multi-Cure adhesives in close-fitting joints.
  • Shadowed-area processing: Provides a secondary cure route where direct light exposure is limited.
  • Multi-substrate surface treatment: Used on metals, ferrite, ceramic, glass, and thermoset plastics within the supported scope.

Applications / Suitable for

  • Activation of Dymax Multi-Cure adhesives
  • Close-fitting structural joints
  • Assemblies with shadowed bond areas
Product Family

DYMAX 535-A-REV-A

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber to Brown
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
37 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Exact-product activator characteristics relevant to application and compatible adhesive processing.

Property Value Unit Method / condition
Appearance Amber-brown As supplied
Solvent / carrier Isopropyl alcohol As supplied
Product function Adhesive cure activator Compatible Dymax Multi-Cure adhesives
Joint geometry Close-gap Applied as a surface treatment
Process role Shadowed-area cure route Where direct light is limited