DYMAX 431-T

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 431-T

Main features

  • Low-Shrinkage Glass Assembly
  • Fast Dissimilar-Material Bonding
  • Heat- and Moisture-Resistant Bonds

Product Description

Dymax 431-T Glass, Plastic and Metal Bonding Adhesive delivers UV- and visible-light cure for bonding glass, plastics, metals, and ceramics. The low-shrinkage formulation is intended for assemblies that need a dimensionally controlled bondline across dissimilar materials. Product characteristics include high-temperature and moisture resistance for bonded components exposed to demanding environments. Fast light cure on accessible bond regions supports efficient assembly without a prolonged thermal cycle. Applications include glass assembly, mixed-material decorative or technical components, and joining the listed substrates where low shrinkage and environmental resistance are important selection factors.

Key features

  • Low-shrinkage bond formation: The formulation limits cure shrinkage for dimensionally sensitive assemblies.
  • Broad dissimilar-material bonding: Bonds glass, plastics, metals, and ceramics within the supported substrate range.
  • Heat and moisture resistance: Cured bonds are positioned for elevated-temperature and moisture exposure.

Applications / Suitable for

  • Glass assembly
  • Dissimilar-material component bonding
  • Plastic, metal, and ceramic joining
Product Family

DYMAX 431-T

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless Transparent Liquid
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.48
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
101 °C
Chemical Properties
Water Absorption
1.3 %

Additional Information

Technical properties

As-supplied / before-processing properties

Exact-product characteristics relevant to cure behavior and dissimilar-material bonding.

Property Value Unit Method / condition
Cure activation UV and visible light Exposed adhesive
Cure response Fast Accessible bond regions
Cure shrinkage Low During cure
Substrate scope Glass; plastics; metals; ceramics Supported bonding surfaces
Technical properties

After-processing / final-state properties

Exact-product final-state characteristics relevant to bonded assemblies under environmental exposure.

Property Value Unit Method / condition
Temperature behavior High-temperature resistant Cured bond
Moisture behavior Moisture resistant Cured bond
Bonded substrate scope Glass; plastics; metals; ceramics Within the listed substrate scope
Dimensional behavior Low-shrinkage bondline After cure