DOWSIL TC-4535

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DOWSIL TC-4535

Main features

  • 3.4 W/(m K) Thermal Interface
  • 60-Minute Working Window
  • 52 Shore 00 Hardness with Vertical-Hold Rheology

Product Description

DOWSIL™ TC-4535 CV Thermally Conductive Gap Filler is a two-part, blue, addition-cure silicone thermal interface material designed to dissipate heat from PCB-mounted electronics to heat sinks or aluminium housings. Parts A and B mix at a simple 1:1 ratio by weight or volume. The mixed material has a typical 205 Pa·s viscosity at 10 s-1, thixotropic index of 3.6, and 60-minute working time at 25°C. Supported cure schedules are 120 minutes at 25°C or 10 minutes at 80°C. Typical cured properties include 3.4 W/m·K thermal conductivity, 52 Shore 00 hardness, 22 kV/mm dielectric strength, and 8 ppm volatile siloxane content from D4 through D10.

Key features

  • Two-part, 1:1 thermally conductive silicone gap filler
  • Typical 3.4 W/m·K thermal conductivity
  • Room-temperature or 80°C heat-accelerated cure
  • Soft 52 Shore 00 cured interface for gap conformity
  • Thixotropic rheology that supports processability and vertical hold
  • Controlled volatile siloxane content of 8 ppm for D4–D10
  • UL 94 V-0 recognition, subject to the current listed formulation and test construction

Applications

  • Engine-control modules
  • Transmission-control units
  • Power-electronics assemblies
  • PCB-to-heat-sink or PCB-to-aluminium-housing thermal interfaces
Product Family

DOWSIL TC-4535

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White/Blue
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.1
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.4 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Physical Properties
Viscosity (Part A)
@10/s 200000 mPa.s
Viscosity (Part B)
@10/s 230000 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
22 kV/mm

Additional Information

Controlled-volatility automotive thermal gap filler

DOWSIL™ TC-4535 CV Thermally Conductive Gap Filler

A blue, two-part silicone thermal interface material designed to transfer heat from PCB-mounted electronics into heat sinks or aluminium housings. The 1:1 system combines soft cured properties, thixotropic vertical hold, controlled volatile siloxane content, and room-temperature or accelerated cure for engine modules, transmission-control units, power electronics, and related assemblies.

Two-part silicone1:1 weight or volume205 Pa·s mixed3.4 W/m·K52 Shore 00
DOWSIL TC-4535 CV Part A and Part B gap filler packaging

DOWSIL TC-4535 CV Part A and Part B gap filler packaging

As supplied and mixed

White Part A, blue Part B, and blue mixed material

Confirm that each component is homogeneous before use. Mix at 1:1 by weight or volume; light-coloured streaks or marbling indicate inadequate mixing.

Property Part A Part B Mixed material
Colour White Blue Blue
Viscosity at 10 s-1 200 Pa·s 230 Pa·s 205 Pa·s
Mix ratio 1:1 by weight or volume
Mixed thixotropic index 3.6, measured as 1 s-1/10 s-1
Working time at 25°C 60 minutes, defined by the TDS as the time for viscosity to double
Processing and cure

Re-homogenise, meter 1:1, mix uniformly, dispense and cure

  • Check both components for minor separation after transportation and re-homogenise where required.
  • Use a static mixer for manual or automated dispensing.
  • Reject or continue mixing if light streaks or marbling remain.
  • Automated airless dispensing can reduce or avoid de-airing.
  • Use only an approved vacuum schedule if void reduction is necessary; the legacy TDS residual-pressure wording is ambiguous.
  • Cure for 120 minutes at 25°C or 10 minutes at 80°C.
  • Allow for component and housing warm-up before starting the heat-cure dwell.
  • Addition cure progresses through deep or confined sections without cure by-products or cure exotherm.
DOWSIL TC-4535 CV process showing re-homogenisation one-to-one metering static mixing dispensing optional de-airing and cure

DOWSIL TC-4535 CV process showing re-homogenisation one-to-one metering static mixing dispensing optional de-airing and cure

Storage and industrial handling

The product-specific TDS reports a 360-day shelf life at 25°C. Store in the original packaging with covers tightly attached, follow special instructions on the label, and use the material by the labelled expiry date. Read the current regional SDS documents and container labels before handling. The product is neither tested nor represented as suitable for medical or pharmaceutical uses.

Thermal and cured properties

Soft gap conformity with thickness-dependent thermal resistance

Thermal conductivity is a bulk property. The published thermal resistance rises with test thickness, so installed performance must be evaluated using the actual gap, pressure, interfaces, contact area, void level, surface condition, and cure.

Property Typical value Test context
Thermal conductivity 3.4 W/m·K Hot Disk, ISO 22007-2.
Thermal resistance at 120 µm 0.45 °C·cm²/W ASTM D5470.
Thermal resistance at 501 µm 1.52 °C·cm²/W ASTM D5470.
Thermal resistance at 1500 µm 4.47 °C·cm²/W ASTM D5470.
Minimum bondline at 0.14 MPa 95 µm CTM 1470 controlled test.
Minimum bondline at 0.42 MPa 61 µm CTM 1470 controlled test.
Hardness 52 Shore 00 ASTM D2240.
Specific gravity, cured 3.1 ASTM D792.
Heat capacity 0.823 J/g·°C at 20°C; 0.962 at 80°C; 1.071 at 150°C ASTM E1269.
Volatile siloxanes D4–D10 8 ppm ASTM F2466 / CTM 0839.
Dielectric strength 22 kV/mm ASTM D149; breakdown property, not working voltage.
Volume resistivity 3 × 1013 ohm-cm ASTM D257.
Dielectric constant / dissipation factor 6.5 / 0.005 at 1 MHz ASTM D150.
Applications and interface design

Bridge PCB assemblies to heat sinks or aluminium housings

TC-4535 CV is directly positioned for engine modules, transmission-control units and power electronics where a soft cured interface must fill irregular gaps and maintain vertical placement. Final qualification should establish the supported gap range, dispensed volume, compression pressure, bondline thickness, housing flatness, void level, wet-out, cure, thermal resistance, vibration, temperature cycling and electrical spacing.

Engine control module using blue silicone gap filler between PCB components and aluminium housing
Engine-control modules

Transfers heat from PCB-mounted electronics to the module housing.

Transmission control unit with blue thermal gap filler contacting an aluminium heat sink
Transmission-control units

Conforms to irregular interfaces while maintaining a soft cured contact.

Power electronics assembly receiving automated meter mix dispensing of blue thermal gap filler
Power electronics

Supports automated meter/mix processing and controlled thermal-interface deposits.

Validate DOWSIL™ TC-4535 CV for your thermal gap and assembly

Krayden can help review gap range, dispense volume, 1:1 metering, static mixer selection, de-airing, vertical hold, pressure, bondline thickness, cure profile, installed thermal resistance, controlled-volatility requirements, temperature cycling and assembly qualification.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers