DOWSIL OS-20

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL OS-20

Main features

  • Immersion, Spray, or Wipe Cleaning
  • Very-Low-Residue Complete Evaporation
  • 0 g/L US VOC-Exempt Solvent

Product Description

DOWSIL™ OS-20 Fluid is a one-part, clear, colorless volatile methylsiloxane fluid used as a precision cleaning agent, surface-preparation solvent and process carrier. It is compatible with most plastics and surface coatings and can be applied by immersion, spray or impregnated wipes. The fluid has a typical dynamic viscosity of 0.8 cP and surface tension of 16.5 dynes/cm at 25°C, supporting easy spreading across complex or multi-material parts. It is an effective solvent for nonvolatile silicone materials and evaporates completely at room temperature with very low residual nonvolatile content, allowing cleaned surfaces to proceed to painting, bonding or sealing after compatibility verification. In the United States, DOWSIL™ OS-20 Fluid is VOC exempt (VOC = 0 g/L) and is certified as a Clean Air Solvent by the California South Coast Air Quality Management District. The product is classified as a flammable liquid.

Key features

  • Multi-material cleaning: Compatible with most plastics and surface coatings and documented for cleaning plastics, metals and other surfaces; verify compatibility on the actual materials.
  • Multiple application methods: Suitable for immersion, spray and impregnated-wipe cleaning according to the part geometry and contamination level.
  • Low-viscosity spreading: Typical dynamic viscosity is 0.8 cP and surface tension is 16.5 dynes/cm at 25°C.
  • Low-residue evaporation: Evaporates completely at room temperature with very low residual nonvolatile content.
  • Silicone solvency and carrier use: Removes nonvolatile silicone materials and can serve as a solvent or carrier for silicone oils and greases.
  • US VOC status: VOC exempt in the United States at 0 g/L and certified as a Clean Air Solvent by the California South Coast Air Quality Management District.

Applications / Suitable for

  • Cleaning plastics, metals, boards and assemblies, components and housings
  • Rinsing parts after cleaning with stronger cleaning agents
  • Aerosol cleaning of industrial optics and spectacle lenses
  • Impregnated wipes for lightly contaminated components
  • Surface preparation before painting, bonding or sealing
  • Solvent or carrier for silicone oils, greases and selected industrial formulations

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.82
Surface Tension
16.5 mN/m
Vapor Pressure
3.9 mmHg
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
152 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
34 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.8 mPa.s

Additional Information

Cleaners and solvents

DOWSIL™ OS-20 Fluid

DOWSIL™ OS-20 Fluid is a one-part volatile methylsiloxane fluid for precision cleaning, surface preparation and carrier use. Its low surface tension and 0.8 cP viscosity support spreading across complex parts, while compatibility with most plastics and surface coatings suits multi-material assemblies. The fluid evaporates completely and can remove nonvolatile silicone contamination before painting, bonding or sealing.

One-part VMS fluid Clear and colorless 0.8 cP at 25°C 16.5 dynes/cm at 25°C 34°C closed-cup flash point US VOC = 0 g/L
Blue droplet graphic used on the supplier product page for DOWSIL OS-20 Fluid

Supplier product-page image for DOWSIL™ OS-20 Fluid.

As supplied

Typical properties

US VOC status
0 g/L
The current supplier page identifies DOWSIL™ OS-20 Fluid as VOC exempt in the United States.
Clean Air Solvent
Certified
The current supplier page states certification by the California South Coast Air Quality Management District.
Ozone depletion
Does not deplete ozone
The technical data sheet describes the DOWSIL™ OS fluid family as not contributing to ozone depletion.

Values below are typical and are not intended for use in preparing specifications. Conditions and methods are shown where available.

Property Value Unit Method / condition
Appearance Clear, colorless liquid — As supplied
Flash point, closed cup 34 °C (94 °F) Closed cup
Boiling point 152 °C (306 °F) At 760 mm Hg
Vapor pressure 3.9 mm Hg At 25°C (77°F)
Dynamic viscosity 0.8 cP At 25°C (77°F)
Specific gravity 0.82 — At 25°C (77°F)
Surface tension 16.5 dynes/cm At 25°C (77°F)
Freezing point -82 °C (-115 °F) Typical value
Drying rate 0.7 relative Butyl acetate = 1; ASTM D-1901
Kauri-butanol value 15 — Typical value
Lower explosive limit 0.9 vol % Flammability property
Upper explosive limit 13.8 vol % Flammability property
Autoignition temperature 350 °C (662 °F) Typical flammability property
Documented packaging 25 L pails; approx. 200 L drums — Availability may vary by region
Use and processing

Cleaning and application

Select equipment and procedures designed for flammable liquids. Verify compatibility on the actual substrate before use, particularly for sensitive coatings or multi-material parts.

Immersion cleaning: Immerse parts with vigorous action to lift soils from surfaces. Use cleaning equipment designed to safely handle flammable liquids.
Spray application: Apply by spray when appropriate to the part geometry and contamination, using explosion-proof ventilation and grounded equipment.
Wipe cleaning: Use tissues or wipes impregnated with the fluid for lightly contaminated components or where more aggressive solvents are unsuitable.
Surface preparation: Allow the fluid to evaporate completely before painting, bonding or sealing. Confirm that the cleaned surface is compatible with the downstream process.
Silicone carrier use: Use as a solvent or carrier for silicone oils and greases or to tailor silicone viscosity. Establish process-specific dilution and performance through evaluation.
Diagram showing immersion, spray and impregnated-wipe cleaning methods for DOWSIL OS-20 Fluid

Supported cleaning methods include immersion, spray and impregnated wipes.

Storage and handling

Store in the original, unopened container at or below 54°C; the documented shelf life is four years from the date of manufacture. Keep containers tightly closed in a cool, well-ventilated area away from heat, sparks, open flames and strong oxidizing agents. DOWSIL™ OS-20 Fluid is a Category 3 flammable liquid and can accumulate static charge. Ground and bond containers and transfer equipment, use non-sparking tools and explosion-proof ventilation, and review the current Safety Data Sheet and container label before handling.

Applications

Cleaning, surface preparation and carrier applications

DOWSIL™ OS-20 Fluid is documented for precision cleaning and carrier uses across parts, assemblies and formulations. Confirm material compatibility and fire-safety controls for the actual process.

Illustration of electronic and industrial parts being prepared for cleaning
Parts and assembly cleaning
Suitable for cleaning plastics, metals, boards and assemblies, components and housings. Low surface tension and compatibility with most plastics and surface coatings support use on complex, multi-material parts; verify compatibility on the actual surfaces.
Illustration of a lens and cleaning wipe for optics cleaning
Optics and wipe-based cleaning
Applications include aerosols for industrial optics and spectacle lenses and impregnated wipes for lightly contaminated components where more aggressive solvents are unsuitable. Use process controls appropriate for a flammable liquid.
Illustration of surface preparation and silicone carrier use before downstream processing
Surface preparation and carrier use
Suitable for removing nonvolatile silicone contamination before painting, bonding or sealing, and for use as a solvent or carrier for silicone oils and greases or in selected industrial formulations. Confirm downstream process compatibility and required dilution.
Next steps

Evaluate DOWSIL™ OS-20 Fluid for your cleaning process

Krayden can help review substrate compatibility, cleaning method, evaporation requirements, flammability controls and whether DOWSIL™ OS-20 Fluid or another volatility grade fits your process. Contact us to discuss part materials, contamination type, equipment, downstream painting or bonding, and sample or supply requirements.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers