DOWSIL OS-2

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL OS2

Main features

Product Description

DOWSIL™ OS-2 Fluid is a one-part, clear, colorless methyl siloxane specialty fluid used as a mild cleaner, silicone solvent and process carrier. Its low surface tension and compatibility with most plastics and surface coatings support cleaning of multi-material parts and delicate coated surfaces, subject to compatibility testing. The fluid can be used to rinse parts after stronger cleaners, applied by spray or immersion, or impregnated into wipes for light contamination. It also serves as a solvent or carrier for silicone oils and greases and as an alternative to hydrocarbon carriers in selected industrial and consumer formulations. After cleaning, it evaporates completely without leaving a silicone trace, supporting subsequent painting or bonding. Typical density is 0.78 g/cm³, dynamic viscosity is 0.59 cP and shelf life is five years at 25°C.

Key features

  • Broad surface compatibility: Compatible with most plastics and surface coatings, including delicate coatings, subject to verification on the actual surface.
  • Multiple cleaning methods: Suitable for immersion, spray application and impregnated wipes according to the part and contamination level.
  • Silicone soil removal: Functions as an effective solvent for nonvolatile silicone materials.
  • Downstream process support: Evaporates completely without leaving a silicone trace so cleaned surfaces can proceed to painting or bonding.
  • Low-viscosity fluid: Typical dynamic viscosity is 0.59 cP, with low surface tension for spreading across surfaces.

Applications / Suitable for

  • Rinsing parts after cleaning with stronger cleaning agents
  • Impregnating wipes where more aggressive solvents cannot be used
  • Carrying materials in selected industrial processes
  • Alternative carrier to hydrocarbon solvents in selected consumer product formulations
  • Solvent or carrier for silicone oils and greases
  • Cleaning contaminated surfaces before painting or bonding

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One-part
Density (g)
0.78 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-5 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.59 mPa.s

Additional Information

Cleaners and solvents

DOWSIL™ OS-2 Fluid

DOWSIL™ OS-2 Fluid is a one-part methyl siloxane specialty fluid for mild cleaning, surface preparation and carrier applications. It is clear and colorless, has low surface tension, and is compatible with most plastics and surface coatings. The fluid can remove nonvolatile silicone contamination and evaporates completely, enabling cleaned surfaces to proceed to painting or bonding after compatibility verification.

One-part specialty fluid Clear and colorless Low surface tension 0.59 cP dynamic viscosity 5-year shelf life at 25°C
Blue droplet graphic used on the supplier product page for DOWSIL OS-2 Fluid

 

As supplied

Typical properties

Values are typical and are not intended as product specifications. Safety-related values support preliminary evaluation and do not replace the current safety data sheet.

Property Value Unit Method / condition
Number of parts One — As supplied
Appearance Clear, colorless liquid — As supplied
Density 0.78 g/cm³ Typical
Dynamic viscosity 0.59 cP CTM 0050; typical
Kinematic viscosity 0.75 cSt Typical
Boiling point 110 °C 760 mmHg; typical
Flash point -3 °C Closed cup
Relative density 0.78 — Water = 1; typical
Water solubility Insoluble — Typical
Auto-ignition temperature 350 °C Typical
Shelf life 5 years Stored at 25°C
Use guidance

Cleaning and application

Select the cleaning method according to soil level, part geometry and surface sensitivity. Verify compatibility on the actual surface before broader use, particularly where multiple materials or delicate coatings are present.

Immersion or spray: Immerse parts with vigorous action or apply the fluid by spray to lift soils from the surface.
Light contamination: Wipe components with tissues impregnated with the fluid where more aggressive solvents are not suitable.
Silicone contamination: Use the fluid as a solvent for nonvolatile silicone materials and as a carrier for silicone oils or greases.
Before painting or bonding: Allow the fluid to evaporate completely before the next process step; cleaned surfaces can then proceed to coating or bonding.
Diagram showing immersion, spray and impregnated-wipe cleaning methods for DOWSIL OS-2 Fluid

Supported cleaning methods include immersion with vigorous action, spray application and wiping lightly contaminated parts with impregnated tissues.

Storage and Handling

Shelf life is five years when stored at 25°C. Keep the container tightly closed in a cool, well-ventilated place away from heat and ignition sources. Because the fluid is a Category 2 flammable liquid and can accumulate static charge, use suitable grounding, bonding, non-sparking tools and explosion-proof ventilation as required by the process. Review the current safety data sheet and container label before handling.

Applications

Applications for DOWSIL™ OS-2 Fluid

DOWSIL™ OS-2 Fluid supports cleaning, surface-preparation and carrier applications where a mild, low-viscosity methyl siloxane fluid is appropriate. Compatibility should be verified on the actual substrates, coatings and process materials before broader use.

Industrial parts being cleaned by immersion or spray with a clear specialty fluid
Parts cleaning and post-cleaning rinse
Parts may be immersed with vigorous action or cleaned by spray to lift soils from their surfaces. The fluid can also be used to rinse parts after stronger cleaning agents or applied through impregnated tissues for lightly contaminated components.
Contaminated component surface being prepared before painting or adhesive bonding
Surface preparation before painting or bonding
The fluid can remove nonvolatile silicone contamination from surfaces. It evaporates completely without leaving a silicone trace, allowing cleaned surfaces to proceed to coating or bonding after compatibility has been verified.
Industrial process equipment using a clear silicone fluid as a solvent or material carrier
Process solvent and carrier applications
The fluid can be evaluated as a carrier in selected industrial processes, as an alternative to hydrocarbon solvents in selected consumer product formulations, and as a solvent or carrier for silicone oils and greases.
Next steps

Evaluate DOWSIL™ OS-2 Fluid for your cleaning process

Krayden can help assess surface compatibility, cleaning method, downstream painting or bonding requirements, and handling considerations for your application. Share the substrates, contamination type, process constraints and intended next step so the technical team can support an appropriate product evaluation.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers