DOWSIL OS-125

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL OS-125

Main features

  • Silicone-Contamination Cleaning Solvent Blend
  • Immersion, Spray, Rinse, or Wipe Cleaning
  • ppm-Level Residual Silicone

Product Description

DOWSIL™ OS-125 is a clear, colorless cleaning solvent composed of hexamethyldisiloxane and acetone. The product is used to remove soils and nonvolatile silicone contamination from surfaces before subsequent painting or bonding. It can be applied by immersion, spray, or wiping with impregnated tissues, depending on the part and contamination level. Its low kinematic viscosity and surface tension support wetting and cleaning across component surfaces, while evaporation leaves only ppm levels of residual silicone. Compatibility should be verified before use, particularly on sensitive plastics that may be affected by acetone.

Key features

  • Silicone-removing solvent blend: Combines hexamethyldisiloxane and acetone for cleaning soils and nonvolatile silicone materials.
  • Low-residue evaporation: Evaporates after cleaning and leaves only ppm levels of residual silicone, allowing cleaned surfaces to be subsequently coated or bonded.
  • Flexible cleaning methods: Suitable for immersion, spray application, rinsing, and use in impregnated cleaning wipes.

Applications / Suitable for

  • Degreasing
  • Rinsing parts
  • Impregnating wipes for cleaning applications
  • Cleaning contaminated surfaces before painting or bonding
Product Family

DOWSIL OS-125

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear, colorless
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.77
Surface Tension
17.2 mN/m

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are not intended for use in preparing specifications. Component-specific transition temperatures are identified in the Method / condition column.

Property Value Unit Method / condition
Appearance Clear, colorless — Typical
Kinematic viscosity 0.5 cSt (mm²/s) Typical
Specific gravity 0.77 — Typical
Surface tension 17.2 dyne/cm Typical
Flash point 5 / -15 °F / °C Acetone component
Freezing point -90 / -68 °F / °C Hexamethyldisiloxane component
Boiling point 133 / 56 °F / °C Acetone component
Shelf life 36 months At 25°C