DOWSIL FS1265

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

DOWSIL FS1265

Main features

  • 100% Active Fluorosilicone Foam Control
  • Chlorinated-Solvent-Insoluble Foam-Control Formulation
  • 300/1,000/10,000 mm^2/s Viscosity Grades

Product Description

DOWSIL™ FS 1265 Fluid is a clear, colorless, 100% active fluorosilicone polymer used for persistent foam control in non-aqueous solvent systems. Its low surface tension, resistance to chemicals and oxidation, and insolubility in chlorinated solvents make it relevant where conventional polydimethylsiloxane fluids dissolve in the process liquid and can promote foam. The fluid can be added directly, prediluted in an acceptable process-compatible solvent, or applied to equipment surfaces that contact rising foam. Three kinematic viscosity grades, 300, 1,000 and 10,000 mm²/s, support different dispersion and solubility requirements; the 1,000 mm²/s grade is recommended for initial testing at a suggested starting concentration of 1–5 ppm.

Key features

  • 100% active fluorosilicone fluid: Provides a concentrated product form for direct addition or controlled predilution.
  • Persistent solvent foam control: Supports antifoaming in chemical and petroleum processes and other non-aqueous systems.
  • Insoluble in chlorinated solvents: Suitable for evaluation where conventional polydimethylsiloxane fluids are soluble and may promote foam.
  • Three viscosity grades: Available at 300, 1,000 and 10,000 mm²/s for balancing dispersion with antifoam efficiency.
  • Low suggested starting level: Begin screening at 1–5 ppm and optimize for the specific foaming system.

Applications / Suitable for

  • Solvent antifoaming in chemical and petroleum processing
  • Reclaiming used chlorinated solvents after dry cleaning, solvent degreasing or solvent extraction
  • Oil and gas separation

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear, colorless liquid
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.3797
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.25

Additional Information

Fluorosilicone fluid and non-aqueous antifoam

DOWSIL™ FS 1265 Fluid

A clear, colorless, 100% active fluorosilicone polymer for persistent foam control in non-aqueous solvent systems. It is insoluble in chlorinated solvents, may be used directly or after predilution, and is available in three viscosity grades. The fluid is also identified by Dow as an ingredient for lubricant formulations.

100% active Clear, colorless fluid 300–10,000 mm²/s Chemical and oxidation resistant High flash point
Approved product image of DOWSIL™ FS 1265 Fluid packaging

 

As-supplied properties

Concentrated fluorosilicone fluid

Active content
100%
Fluorosilicone polymer supplied as an active fluid rather than an aqueous emulsion.
Appearance
Clear, colorless
Liquid appearance as supplied.
Kinematic viscosity grades
300 / 1,000 / 10,000 mm²/s
Use grade selection to balance dispersion with solubility and foam-control efficiency.
Grade comparison

Viscosity grade selection

Increasing viscosity lowers solubility in the foaming solvent and can increase antifoaming efficiency, but it also makes thorough dispersion more difficult. Select the lowest viscosity grade that provides acceptable foam control; use the 1,000 mm²/s grade for initial testing.

Viscosity grade Specific gravity at 25°C Refractive index at 25°C Selection context
300 mm²/s 1.25 1.3797 Lower-viscosity option for easier dispersion; confirm that foam control is sufficient in the target system.
1,000 mm²/s 1.27 1.3802 Recommended starting grade for initial foam-control testing.
10,000 mm²/s 1.30 1.3809 Lower solubility can improve antifoaming efficiency, with greater effort required for complete dispersion.

Typical values are not intended for specification writing. Specific gravity: ASTM D1298-24. Refractive index: ASTM D1218-21.

Processing

Application and dosage

Use the fluid as supplied or predilute it in a process-compatible solvent to improve distribution. Direct addition to the liquid system is the usual method. It may also be wiped onto a vat rim or onto a screen suspended above the liquid so rising foam contacts the treated surface.

Initial test grade
1,000 mm²/s
Starting concentration
1–5 ppm
Product form
Use neat or prediluted
1. Characterize the foaming system
Confirm the solvent composition, foam severity, process temperature and practical mixing or dispersion capability before selecting a grade.
2. Choose the delivery method
Add directly, predilute in an acceptable solvent, or use controlled surface contact on equipment that rising foam reaches.
3. Begin at a low level
Start testing at 1–5 ppm and ensure the fluid is dispersed thoroughly before increasing concentration.
4. Optimize grade and dose
Use the lowest viscosity grade that provides satisfactory foam control, then confirm performance under representative process conditions.
Storage and handling

Store at or below 40°C (104°F) in the original unopened container. Under these conditions, the usable life is 48 months from the date of production. Diluted solutions may lose performance after more than four weeks of storage. Review the current product safety documentation and container label before handling. Package options include 550 lb drums, 25 kg pails, 5 kg and 1 kg packs, and 250 cc samples; confirm regional availability.

Applications

Supported foam-control applications

Application fit depends on the foaming solvent, dispersion method, grade and dose. Use representative system testing to establish the operating window.

Chemical or petroleum process vessel with controlled non-aqueous solvent foam
Chemical and petroleum solvent processing
Applications include solvent antifoaming where persistent foam control is required in chemical or petroleum operations.
Closed solvent-recovery equipment used to reclaim chlorinated process solvent
Chlorinated-solvent reclaiming
Suitable for reclaiming used chlorinated solvents after dry cleaning, solvent degreasing or solvent extraction operations.
Oil and gas separation equipment showing liquid and gas phase separation
Oil and gas separation
May be used for foam control during oil and gas separation, subject to process-specific grade and dosage testing.
Product resources

Foam-control selection guides

These supplier guides provide broader portfolio context for application screening. Product-specific properties and use guidance on this page should remain the basis for evaluating DOWSIL™ FS 1265 Fluid.

Silicone Antifoams for Oil & Gas Processing — Selection Guide
A portfolio selection guide for comparing silicone foam-control products and application considerations across oil and gas processing. Use it alongside product-specific grade and dosage testing.
View selection guide
Silicone Antifoams for Chemical Processing — Selection Guide
A broader reference for evaluating silicone antifoams in chemical processing systems. It supports portfolio screening; final product choice should be confirmed in the actual foaming medium.
View selection guide
Silicone Antifoams for Metal & Glass Working Fluids — Selection Guide
A portfolio guide for foam-control evaluation in metal- and glass-working fluids. Use it to compare candidate technologies and retain system-specific testing for product qualification.
View selection guide
Next steps

Evaluate DOWSIL™ FS 1265 Fluid for your foam-control process

Share the solvent system, foam behavior, process temperature, available dispersion equipment and target dosing range with Krayden. Our technical team can support a controlled screening plan for viscosity grade, predilution approach and starting concentration before production qualification.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers