Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL EA6052

Main features

  • Temperature-Controlled Heat Cure
  • Five-Hour Working Window
  • UV Light Bonding Cure

Product Description

DOWSIL™ EA-6052 Fast Low-Temp Cure Adhesive Kit is a black, flowable, two-part addition-cure silicone adhesive mixed 1:1 by weight or volume. Its temperature-controlled heat cure gives manufacturers a choice of 60 minutes at 90°C, 30 minutes at 125°C, or 10 minutes at 150°C, while a typical five-hour working time at 25°C supports dispensing and assembly operations. The mixed material can flow, fill, or self-level after dispensing and includes a UV indicator for inspection. Typical cured performance includes 4.7 MPa tensile strength, 170% elongation, Shore A 48 hardness, and 4.9 MPa unprimed lap shear to aluminum. Applications include sealing lids and housings, attaching baseplates, gasketing, and connector sealing.

Key features

  • Temperature-controlled cure: Typical heat-cure schedules are 60 minutes at 90°C, 30 minutes at 125°C, or 10 minutes at 150°C.
  • Two-part 1:1 system: Parts A and B are mixed 1:1 by weight or volume, with a typical five-hour working time at 25°C.
  • Flowable dispensing: The mixed adhesive can flow, fill, or self-level and may be applied by manual or automated needle dispense.
  • UV inspection indicator: Supports visual inspection after dispensing.
  • Cured mechanical profile: Typical values include 4.7 MPa tensile strength, 170% elongation, Shore A 48 hardness, and 4.9 MPa lap shear to aluminum.

Applications / Suitable for

  • Sealing lids and housings
  • Attaching baseplates
  • Gasketing
  • Connector sealing

Technical Specifications

Physical Properties
Viscosity (Part B)
41,425 mPa.s
General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.24
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
170 %

Additional Information

Electronics assembly silicone adhesive

DOWSIL™ EA-6052 Fast Low-Temp Cure Adhesive Kit

DOWSIL™ EA-6052 is a black, flowable two-part silicone adhesive for sealing and attachment tasks in electronic assemblies. A 1:1 mix ratio, five-hour working time at 25°C, temperature-controlled heat cure and UV inspection indicator support flexible dispensing and assembly workflows, including lids, housings, baseplates, gaskets and connectors.

Two-part addition cure 1:1 mix by weight or volume 5-hour working time at 25°C Flowable and self-leveling UV inspection indicator Black
DOWSIL EA-6052 Fast Low-Temp Cure Adhesive Kit packaging

Product image for DOWSIL™ EA-6052 Fast Low-Temp Cure Adhesive Kit.

As-supplied properties

Mix ratio
1:1
Combine Parts A and B by weight or volume after separately mixing each component.
Working time
5 hr at 25°C
Typical pot life after mixing supports dispensing and assembly before heat cure.
Typical as-supplied properties; values are not intended for specification use.
Property Value Unit Method / condition
Color Black — As supplied / mixed system
Part A viscosity 39,800 mPa·s Typical
Part B viscosity 41,425 mPa·s Typical
Mixed viscosity 40,600 mPa·s Typical
Mix ratio 1:1 By weight or volume Parts A and B
Working time 5 hr Typical at 25°C
Application method Manual or automated needle dispense — Product application method
Processing

Mixing, dispensing and cure

This two-part system requires uniform component preparation, controlled 1:1 mixing and a heat-cure schedule selected for the assembly process. Surface cleanliness, cure compatibility and air management should be verified before production.

Mixing ratio: 1:1 by weight or volume; mix Parts A and B separately before combining.
Working time: Typical 5 hours at 25°C after mixing.
Cure schedule: 60 minutes at 90°C; 30 minutes at 125°C; or 10 minutes at 150°C.

Application sequence

Stage 1
Prepare surfaces and verify compatibility
Clean and degrease the bonding surfaces, and use light abrasion where practical. Acetone or isopropyl alcohol can serve as a final wipe but should not be relied on alone to remove oils. Test adhesion and cure compatibility on the actual materials; organotin catalysts, sulfur-containing materials, unsaturated hydrocarbon plasticizers and some solder-flux residues can inhibit addition cure.
Stage 2
Prepare and mix the components
Mix Parts A and B separately to redistribute filler, then combine them 1:1 by weight or volume until the blend is uniform. Light-colored streaks or marbling indicate inadequate mixing. For air-sensitive assemblies, de-air at 28–30 in Hg vacuum; automated mix-and-dispense equipment is recommended for fast-cure processing.
Stage 3
Dispense, assemble and heat cure
Dispense manually or automatically through a needle, assemble the parts, and heat cure for 60 minutes at 90°C, 30 minutes at 125°C, or 10 minutes at 150°C. Increasing cure temperature and/or cure time can improve ultimate adhesion.
Storage and handling

Store at 25°C and use before the date shown on the product label. Typical shelf life is 12 months at 25°C. Review the current Safety Data Sheet and container label before handling.

Cured properties

Tensile strength
4.7 MPa (685 psi)
Typical cured tensile strength.
Unprimed lap shear to aluminum
4.9 MPa (710 psi)
Typical result on aluminum; substrate, preparation and cure conditions affect adhesion.
Typical cured properties; values are not intended for specification use and adhesion is configuration-dependent.
Property Value Unit Method / condition
Specific gravity 1.24 — Typical, cured
Tensile strength 4.7 (685) MPa (psi) Typical, cured
Elongation 170 % Typical, cured
Tensile modulus 2.8 (400) MPa (psi) Typical, cured
Tear strength, Die B 34 (50) N/cm (ppi) Typical, cured
Durometer 48 Shore A Typical, cured
Unprimed lap shear to aluminum 4.9 (710) MPa (psi) Typical, aluminum substrate
Product resource

Product resources

Dow Adhesives and Sealants Selection Guide
A portfolio-level reference covering Dow silicone adhesive and sealant technologies, processing options and typical selection data. Use the current product-specific information on this page when evaluating DOWSIL™ EA-6052.
Next steps

Evaluate DOWSIL™ EA-6052 for your assembly process

Krayden can help review substrate compatibility, dispensing approach, cure-temperature tradeoffs and the mechanical properties relevant to lid sealing, baseplate attachment, gasketing or connector sealing. Contact our team to discuss samples, process evaluation and product selection for your assembly.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers