DOWSIL EA-2626

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL EA-2626

Main features

  • Fast Adhesive Cure
  • Non-Sag Placement Control
  • Robust Cured Mechanical Properties

Product Description

DOWSIL™ EA-2626 Adhesive is a two-component, room-temperature curing, non self-leveling adhesive. It utilizes a neutral alkoxy cure system and maintains a paste consistency. This adhesive is developed to provide durable adhesive sealing for components which exhibit different thermal expansion rates, or where fast cure requirements make one-part room temperature cure adhesives inappropriate.

Product Key Features

  • Two-Component Fast Cure - cures rapidly at room temperature with a fast cure in-depth, unlike typical outside-inward moisture cure adhesives, allowing for rapid handling of bonded components.
  • Mix Ratio - designed to be used with SILASTIC™ Q3-3636 Catalyst in a mix ratio of 100 parts base to 13 parts catalyst by weight.
  • Non-Sag Rheology - features a non self-leveling, paste consistency that ensures the material remains in place during application.
  • Robust Mechanical Profile - cures to deliver a Shore A hardness of 43 to 45, a tensile strength greater than 1.9 MPa, and an elongation at break of more than 200%.
  • Environmental & Heat Resistance - offers excellent weathering, U.V., and heat resistance up to 190°C, alongside good resistance to hot and humid conditions.

Applications

This adhesive provides good, durable adhesion to a range of substrates including plastics, metals, and glass, making it highly effective for both automotive and appliance manufacturing[cite: 1742].

  • Automotive Lighting - typically used in automotive manufacturing for bonding polycarbonate or glass lenses to the reflector housings of headlamps and fog lamps.
  • Appliance Assembly - serves as a perfect solution in appliance manufacturing, especially for oven and ceramic hob assembly, seamlessly bonding glass to metal, painted metal, or plastic.
  • Dissimilar Materials - provides durable sealing for components that exhibit different thermal expansion rates.

Technical Specifications

General Properties
Color
The color
A/B: White/ Gray, Special black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
A/B (Gray, Special Black): 1.31/1.00,1.04
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.1 hours
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
>200 %

Additional Information

Two-Component Fast Room Temperature Cure Adhesive

DOWSIL™ EA-2626 Adhesive

DOWSIL™ EA-2626 Adhesive is a two-component, non-self-leveling silicone adhesive system engineered to deliver a fast room-temperature cure in-depth, rather than curing outside-inward like typical moisture-cure adhesives. Utilizing a neutral alkoxy cure system, it consists of DOWSIL™ EA-2626 Base paired with SILASTIC™ Q3-3636 Catalyst (available in Grey or Special Black). This high-performance adhesive is specifically developed to provide durable, elastic structural bonding and sealing for components exhibiting different thermal expansion rates, offering rapid handling capabilities without the need for temporary storage infrastructure.

100:13 mix ratio by weight 6 to 9 min snap time Fast homogeneous depth cure Heat resistance to 190°C
Contact Us

Typical values only. Performance profiles are measured at standard ambient conditions of 23°C unless otherwise indicated.

DOWSIL EA-2626 Adhesive product package
DOWSIL™ EA-2626 Adhesive

Key Features

  • Two-component room-temperature cure executes a fast, thorough depth cure independent of joint thickness.
  • Non-self-leveling thixotropic paste consistency resists running or slumping, remaining under 2 mm of vertical flow.
  • Cures smoothly to form a highly resilient, flexible silicone rubber with robust weathering and UV stability.
  • Durable, unprimed adhesion profiles build rapidly onto glass, ceramics, metals, and selected automotive plastics.
  • High thermal resistance safely withstands exposure conditions continuously up to 190°C.
  • Excellent hot and humid aging performance, maintaining joint integrity after 7 days immersion in water at 70°C.

Processing Summary

Mix Proportions: Calibrated for a precise mix ratio of 100 parts base to 13 parts catalyst by weight. Volumetric pump parameters compute to 5.7:1 for the Grey catalyst and 5.9:1 for the Special Black catalyst.
Working & Tack-Free Windows: Exhibits a fast inline working snap time of 6 to 9 minutes at 23°C. The material develops a tack-free surface state within a quick 11 to 18-minute window.
Rapid Handling Turnaround: Deep cross-linking progresses fast at ambient room conditions, enabling bonded parts and assemblies to be transferred or handled within 10 to 120 minutes.
Cure Acceleration: Ambient moisture cures eliminate oven operations, but the cure and adhesion strength build rate can be further quickened by applying moderate heat at 60-70°C for 10 minutes.
Handling and Application Guidance

Process Notes 

Storage and Shelf Life
  • Store DOWSIL™ EA-2626 Base in unopened original containers at or below 32°C to retain a 12-month shelf life.
  • Store SILASTIC™ Q3-3636 Catalysts (Grey and Special Black) in unopened original containers at or below 25°C to realize a 5-month shelf life.
  • Keep containers tightly closed to prevent atmospheric moisture from contaminating the materials.
Surface Preparation
  • All bonding joint faces must be thoroughly clean, dry, and cleared of dust, dirt, or extraneous matter.
  • Degrease boundaries using pure industrial solvents like isopropyl alcohol, acetone, or methyl ethyl ketone (MEK).
  • Low surface energy substrates like polypropylene (PP) can achieve excellent hold via localized plasma or flame treatment.
  • Avoid using acetone or IPA alone if heavy processing oils are present, as they do not remove oils effectively.
Equipment and Mixing
  • Robotic meter/mix/dispense machinery must be fitted with precision gear or piston metering pumps for base and catalyst channels.
  • Dispense through an engineered static or dynamic mixing element array to ensure uniform composition.
  • Watch the extrusion profile closely; the presence of light-colored streaks or marbling indicates inadequate mixing.
  • Automated airless dispense equipment configuration is highly recommended to eliminate or minimize inline de-airing steps.
Typical Properties

Engineering Data for DOWSIL™ EA-2626

Uncured Component Characteristics (As Supplied)

Property Parameter EA-2626 Base Q3-3636 Catalyst Grey Q3-3636 Catalyst Special Black Standard / Notes*
Appearance / Color White paste Grey Special Black CTM 0176
Viscosity (mPa·s) 205,000 18,000 - 48,000 350,000** (ca.) ASTM D1084 /
Penetration test utilized for Black
Specific Gravity 1.36 1.00 1.04 ASTM D1475

*Materials were tested according to Dow Corporate Test Methods (CTM), which in most cases are similar to the ASTM (American Society for Testing and   Materials)standards listed above
**A penetration test is used to measure consistency of Catalyst Special Black. Value 180–460 mm/10

Mixed & Cured Elastomer Performance Characteristics

Elastomeric Property Parameter With Grey Catalyst With Special Black Catalyst Test Standard / Condition Basis
Working Time (Snap) 6 - 9 minutes 6 - 9 minutes Measured at 23°C
Tack-Free Time 11 - 18 minutes 11 - 18 minutes Measured at 23°C
Flow (Slump Resistance) < 2 mm < 2 mm ASTM D1475
Specific Gravity (Cured) 1.32 1.33 ASTM D1475
Color (RAL Code Equivalent) 7000 7021 -
Durometer Hardness 43 Shore A 45 Shore A Cured 7 days @ 23°C, 2mm sheets
(ASTM D2240)
Tensile Strength > 1.9 MPa > 1.9 MPa Cured 7 days @ 23°C, 2mm sheets
(ASTM D412)
Elongation at Break > 200 % > 200 % Cured 7 days @ 23°C, 2mm sheets
(ASTM D412)

Adhesion strength metrics & Lap Shear Performance

Testing Format Dwell Profile: 24 hours cure at 23°C

Substrate Interface Combo Matrix Lap Shear Value (Grey / Black) Cohesive Failure Rate (CF %)
Clear Polycarbonate (PC) Verified Bond 100% / 100%
Polycarbonate / Treated Polypropylene (PC/PP*) > 1.0 MPa / > 1.0 MPa 100% / 100% (*PP treated with plasma)
Polycarbonate / Glass (PC/Glass) > 1.0 MPa / > 1.0 MPa 100% / 100%
PBT-ASA Plastic Blend / Glass > 1.0 MPa / > 1.0 MPa 100% / 100%
Applications

Where DOWSIL™ EA-2626 Fits

Automotive headlamp assembly line bonding lens to housing
Automotive Lighting Glazing
Perfectly optimized for vehicular headlamp and fog lamp assembly configurations where standard one-part moisture cure sealants restrict high inline throughput.
  • Bonds polycarbonate or glass lenses fluid-tight.
  • Mounts lenses strongly onto plastic reflector housings.
  • Absorbs severe operational vibration without line hold failure.
Domestic kitchen appliance ceramic hob assembly
Appliances & Ceramic Hobs
Delivers premium structural bonding seals for modern white goods, domestic ovens, and professional kitchen hobs.
  • Secures structural glass elements directly to metals.
  • Bonds glass cleanly onto painted metals or plastic frameworks.
  • Withstands rigorous daily high-heat exposure profiles.
Flexible joint sealing between dissimilar sub-assembly surfaces
Dissimilar Material Interfaces
Specially tailored to serve as a durable, stress-relieving sealant between parts demonstrating widely different linear thermal expansion rates.
  • Maintains 100% cohesive failure boundaries across variant surfaces.
  • Compensates for relative dimensional shifts under thermal flux.
  • Non-sag consistency forms uniform seals on vertical runs.
Package & Support

Standard Packaging & Technical Help

Standard Container Sizes
  • Available across different standard industrial protective container sizes matching commercial hardware.
  • Packaged independently as clean DOWSIL™ EA-2626 Base and high-shear active catalysts.
  • Logistics configurations maintain high seal metrics to shield elements from room humidity.
Technical Help Capabilities
  • Calibrating custom volumetric mixing ratios from weight guidelines to align pump mechanics.
  • Auditing component layout lines to identify and rule out potential chemical addition-cure inhibitors.
  • Advising on surface plasma or flame activation methods for difficult substrates like treated Polypropylene.
  • Coordinating lab-scale substrate evaluations to establish minimum line cure parameters.
Technical Guidance

Tips and Troubleshooting

Issue Recommended Action
Light-colored streaks or marble patterning visible in the compound bead
  • This pattern denotes inadequate or non-homogeneous product mixing across base and catalyst lines.
  • Ensure components are blended thoroughly at a 100:13 weight ratio or specified volume indices (5.7–5.9:1).
  • Inspect meter/mix equipment configuration; evaluate static mixing element counts or dynamic heads.
Extended handling wait windows or slowdown in expected cure tracking speeds
  • Check material temperature values just prior to and following the mechanical mixing loop.
  • Maintain ambient application environments above standard factory levels to normalize cross-linking.
  • Introduce moderate inline heat acceleration at 60-70°C for 10 minutes to quicken handling throughput.
Adhesion tracking breakdown or low lap shear metrics on low-energy plastics
  • Unprimed structural bonds will not stick successfully onto non-reactive surfaces like raw Polypropylene.
  • Thoroughly clear joint boundaries using pure isopropyl alcohol, acetone, or MEK solvents.
  • Incorporate verified surface activation techniques such as localized inline flame or plasma treatment.
Next Steps

Ready to Qualify DOWSIL™ EA-2626?

Share your manufacturing performance, design architecture, and throughput constraints with us. Tell us about your specified substrate materials, planned cycle line speeds, and fluid dispensing hardware. Our global technical networks are prepared to put our silicon-based materials experience and processing knowledge to work for your factory floor.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers