DOWSIL 983

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 983

Main features

  • Two-Part Structural Glazing Silicone
  • +/-25% ASTM C719 Movement
  • 10 to 25-Minute Working Window

Product Description

DOWSIL™ 983 Structural Glazing Sealant is a two-part, neutral-cure RTV silicone sealant for factory-applied structural glazing and weathersealing in curtainwall production. The base and curing agent form a non-sag material that cures at room temperature into a high-modulus, flexible silicone rubber. The product provides unprimed adhesion to most common construction materials and is compatible with reflective glass, laminated glass, and most insulating glass configurations. It meets ASTM C1184 for structural silicone sealants and ASTM C719 Class 25 for movement capability. Structural applications require project-specific review by Dow technical staff.

Key features

  • Dual structural and weatherseal capability: Supports factory glazing applications requiring structural attachment and ±25% weatherseal movement performance.
  • Structural glazing compliance: Passes ASTM C1184 Structural Silicone Sealant Specification and meets ASTM C719 Class 25.
  • Controlled two-part processing: Provides a 10–25 minute working time and less than 5 mm flow or sag when mixed at the documented ratio.

Applications / Suitable for

  • Factory structural glazing
  • Curtainwall production
  • Unitized glazing systems
  • Combined structural and weatherseal joints

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.36
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
120 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties for the separately supplied base and curing agent and for the catalyzed material. Values are not intended for specification preparation.

Property Value Unit Method / condition
Color and physical form White paste — Base, as supplied
Specific gravity 1.36 — ASTM D1475; base, as supplied
Color and physical form Black or gray paste — Curing agent, as supplied
Specific gravity 1.055 black; 1.00 gray — ASTM D1475; curing agent, as supplied
Mix ratio 9:1 by volume Base to curing agent; standard pump ratio. Adjustable from 8:1 to 10:1 by volume
Working time 10–25 minutes Catalyzed at 9:1 base-to-curing-agent ratio by volume
VOC content <18 g/L Mixed black or gray; value may depend on mixing ratio
Flow / sag <0.2 (<5) in (mm) ASTM D2202; catalyzed material

After-processing / final-state properties

Typical cured properties and specification test results. Mechanical values were measured after seven days at 77°F and 50% relative humidity unless otherwise noted.

Property Value Unit Method / condition
Durometer hardness 30–40 Shore A points ASTM C661; after 1 day at 77°F and 50% RH
Durometer hardness 35–45 Shore A points ASTM C661; after 7 days at 77°F and 50% RH
Ultimate tensile strength 300 (2.0) psi (MPa) ASTM D412; after 7 days at 77°F and 50% RH
Tensile strength at 25% strain 50 (0.35) psi (MPa) ASTM C1135; after 7 days at 77°F and 50% RH
Ultimate tensile strength 160 (1.1) psi (MPa) ASTM C1135; after 7 days at 77°F and 50% RH
Ultimate elongation 120 % ASTM C1135; after 7 days at 77°F and 50% RH
Movement capability ±25 % ASTM C719 Class 25
Structural silicone sealant specification Passes — ASTM C1184