DOWSIL 92-023

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL 92-023

Main features

  • Adhesion-Promoting Surface Treatment
  • Improved Inhibition Resistance in Addition-Cure Silicone Systems
  • 1 to 2-Hour Cure Window

Product Description

DOWSIL™ 92-023 Primer is a clear, heptane-dispersed adhesion primer that enhances bonding of room-temperature-vulcanizing and heat-cure silicones to a range of prepared surfaces. It is suitable for use on many metals, ceramics, glass, wood, masonry, and structural plastics and can also improve the inhibition resistance of addition-cure silicone systems. The ready-to-use liquid is applied as a very light, even coat by wiping, dipping, or spraying. After application, the primer reacts with atmospheric moisture and is generally cured at room temperature for 1–2 hours before the silicone elastomer is applied.

Key features

  • Silicone adhesion promotion: Enhances bonding of RTV and heat-cure silicones to properly prepared substrates.
  • Addition-cure compatibility: Improves inhibition resistance when used with addition-cure silicone systems.
  • Broad substrate scope: Applicable to many metals, ceramics, glass, wood, masonry, and structural plastics.
  • Multiple application methods: May be applied in a light, even coat by wiping, dipping, or spraying.
  • Room-temperature cure: Generally cures for 1–2 hours at 20–90% relative humidity before silicone application.

Applications / Suitable for

  • Promoting RTV and heat-cure silicone adhesion to prepared metal surfaces
  • Priming glass and ceramic surfaces before silicone bonding or sealing
  • Treating compatible wood, masonry, and structural-plastic surfaces before silicone application
  • Processes requiring improved inhibition resistance with addition-cure silicones

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-13 °C

Additional Information

Primers and adhesion promoters

DOWSIL™ 92-023 Primer

A clear, heptane-dispersed primer that enhances the adhesion of RTV and heat-cured silicones to a range of bonding surfaces. DOWSIL™ 92-023 Primer is applied as a thin, uniform coating and also improves inhibition resistance in addition-cured silicone systems.

Clear liquid primer Heptane-dispersed For RTV and heat-cured silicones Multiple application methods 18-month typical shelf life
DOWSIL 92-023 Primer in its commercial product container

DOWSIL™ 92-023 Primer for preparing bonding surfaces before silicone application.

Product characteristics

As-supplied properties

Typical values are provided for product evaluation and are not intended as guaranteed specifications.

Property Value Unit Condition or context
Product form Clear liquid primer — Adhesion-enhancing material dispersed in heptane
Flash point -13 °C Equivalent reported value: 9°F
Volatile organic content 681 g/L OS Fluid non-exempt basis
Shelf life 18 months Typical value at 25°C; observe the labeled use-before date
Processing

Surface preparation, application, and cure

Clean and degrease the bonding surface and allow all cleaning solvents to evaporate. Apply DOWSIL™ 92-023 Primer in a very light, uniform coating by wiping, dipping, or spraying. Excess primer should be removed because over-application may produce a white, chalky surface. Allow the primer to cure fully before applying the silicone material.

Surface preparation
Clean and dry
Remove oils and contaminants. Light abrasion may improve cleaning and increase the available bonding area.
Application methods
Wipe, dip, or spray
Use a very light and even coat to achieve complete wetting without excessive buildup.
Typical primer cure
1–2 hours
At room temperature and 20–90% relative humidity; lower temperature or humidity requires more time.
Heat acceleration
Below 60°C
Mild heat may accelerate cure, but temperatures above 60°C are not recommended.

Application, dilution, and storage guidance

When wiping, replenish the cloth with fresh material every 3–5 minutes. For dip or spray application, dilution by a factor of 2–4 with additional suitable solvent may help avoid excessive buildup. Store below 32°C with containers tightly closed and moisture exposure minimized. Do not use material that develops a milky appearance or substantial white precipitate, which can indicate moisture contamination.

Applications

Product applications

DOWSIL™ 92-023 Primer may be used to prepare compatible bonding surfaces before the application of RTV or heat-cured silicone materials. Customers should verify adhesion and process conditions on the intended substrate and assembly.

Metal, ceramic, and glass parts prepared with primer before silicone bonding
Metal, ceramic, and glass bonding
Surface preparation for silicone bonding to commonly used nonporous substrates, including metals, ceramics, and glass.
Electronic board, connector, and housing surfaces being prepared before silicone application
Boards, components, and housings
Priming of suitable surfaces in electronic boards, assemblies, components, connectors, and housings before applying addition-cured silicone materials.
Wood, masonry, and structural plastic surfaces prepared for bonding with silicone
Wood, masonry, and structural plastics
Preparation of suitable wood, masonry, and structural-plastic substrates where improved silicone adhesion is required and confirmed through application testing.
Product resources

Primer and application selection resources

Use these supporting guides to review primer selection, surface preparation considerations, and silicone-material options for demanding electronics and aerospace applications.

Selection guide

DOWSIL™ primers, prime coats, and adhesion promoters

Review Dow primer and adhesion-promoter technologies, their substrate considerations, and their role in preparing bonding surfaces for silicone materials.

Open the primer and adhesion promoter guide

Application selection guide

Dow aerospace, defense, and avionics selection guide

Explore Dow silicone-material categories and selection considerations for aerospace, defense, and avionics assemblies, including bonding and surface-treatment applications.

Open the aerospace and avionics selection guide

Next steps

Technical support for DOWSIL™ 92-023 Primer

Need help evaluating DOWSIL™ 92-023 Primer for a specific silicone, substrate, surface-preparation method, or production process? Krayden can help review primer selection, application conditions, cure requirements, and the adhesion tests needed for your assembly.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers